Precipitated Phases and Corrosion Behavior in the Dissimilar Alloy 690-SUS 304L Joints Formed by EBW and GTAW

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effects of Nb on the Microstructure and Elevated-Temperature Mechanical Properties of Alloy 690-SUS 304L Dissimilar Welds

The purpose of this paper was to investigate the effects of Nb on the microstructure and elevated-temperature mechanical properties of Alloy 690-SUS 304L dissimilar welds. The results show that the welds were dominant with dendrites and interdendritic phases. In the low Nb welds, the main interdendritic phases were Nb-rich and Al-Ti-rich phases. Cr-carbides were precipitated along the grain bou...

متن کامل

Corrosion behavior of dissimilar welded joint between Inconel 617 alloy and A387-Gr.11 low-alloy steel

In this study, Inconel 617 alloy was welded to A387-Gr.11 low-alloy steel using ER309L filler metal via gas tungsten arc welding (GTAW). First, the corrosion behavior of Inconel 617, A387-Gr, and the weld metal was evaluated by the Tafel polarization test and electrochemical impedance spectroscopy (EIS) in acidic (H2SO4), neutral (NaCl), and combined (H2SO4 + NaCl) solution at ambient temperatu...

متن کامل

Corrosion behavior of dissimilar welded joint between Inconel 617 alloy and A387-Gr.11 low-alloy steel

In this study, Inconel 617 alloy was welded to A387-Gr.11 low-alloy steel using ER309L filler metal via gas tungsten arc welding (GTAW). First, the corrosion behavior of Inconel 617, A387-Gr, and the weld metal was evaluated by the Tafel polarization test and electrochemical impedance spectroscopy (EIS) in acidic (H2SO4), neutral (NaCl), and combined (H2SO4 + NaCl) solution at ambient temperatu...

متن کامل

Creep behavior and in-depth microstructural characterization of dissimilar joints

The 700 °C power plants currently under development will utilize Ni-base alloys such as alloy 617 for components to be operated at temperatures >650 °C. Due to economic reasons for components or parts of components which are subjected to temperatures <650 °C, 2% Cr or 9-12% Cr steels is used, depending on the required mechanical properties. This makes the dissimilar joining of Ni-base alloys an...

متن کامل

Galvanic Corrosion between Alloy 690 and Magnetite in Alkaline Aqueous Solutions

The galvanic corrosion behavior of Alloy 690 coupled with magnetite has been investigated in an alkaline solution at 30 °C and 60 °C using a potentiodynamic polarization method and a zero resistance ammeter. The positive current values were recorded in the galvanic couple and the corrosion potential of Alloy 690 was relatively lower. These results indicate that Alloy 690 behaves as the anode of...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MATERIALS TRANSACTIONS

سال: 2007

ISSN: 1345-9678,1347-5320

DOI: 10.2320/matertrans.mer2007010