Powder Metallurgical Tungsten Fiber-Reinforced Tungsten
نویسندگان
چکیده
منابع مشابه
Solubilization of cobalt from tungsten carbide–cobalt powder
Several reviews of the toxicology of cobalt, including toxicokinetic aspects, are available (IARC, 1991; Midtgård & Binderup, 1994; Lauwerys & Lison, 1994; Lison, 1996; Barceloux, 1999). This section will focus on the toxicokinetic data published since the previous IARC evaluation (1991) and potentially relevant for cancer. Particular emphasis will be put on studies that examined the fate of in...
متن کاملTungsten disulfide nanotubes reinforced biodegradable polymers for bone tissue engineering.
In this study, we have investigated the efficacy of inorganic nanotubes as reinforcing agents to improve the mechanical properties of poly(propylene fumarate) (PPF) composites as a function of nanomaterial loading concentration (0.01-0.2 wt.%). Tungsten disulfide nanotubes (WSNTs) were used as reinforcing agents in the experimental group. Single- and multi-walled carbon nanotubes (SWCNTs and MW...
متن کاملTungsten toxicity.
There is emerging evidence that tungsten has toxic health effects. We summarize the recent tungsten toxicity research in this short review. Tungsten is widely used in many commercial and military applications because it has the second highest melting temperature of any element. Consequently, it is important to elucidate the potential health effects of tungsten.
متن کاملSeed growth of tungsten diselenide nanotubes from tungsten oxides.
We report growth of tungsten diselenide (WSe2) nanotubes by chemical vapor deposition with a two-zone furnace. WO3 nanowires were first grown by annealing tungsten thin films under argon ambient. WSe2 nanotubes were then grown at the tips of WO3 nanowires through selenization via two steps: (i) formation of tubular WSe2 structures on the outside of WO3 nanowires, resulting in core (WO3)-shell (...
متن کاملRefinement of the T466 Prototype Tungsten/Scintillating Fiber Electromagnetic Calorimeter
In April 2003, UCLA researchers conducted test run T466 at the Stanford Linear Accelerator Center with their newly designed electromagnetic calorimeter towers composed of tungsten powder and scintillating fibers. The prototype’s energy resolution, uniformity of response, and linearity were measured using an electron beam with a momentum of up to 10 GeV. The measured energy resolution was 17%/ √...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science Forum
سال: 2015
ISSN: 1662-9752