Micrometric Growth of V2O5Hexagonal Nano-plates as an Active Material for Lithium Ion Battery Cathode Electrode

This manuscript reports the synthesis of V2O5 nanostructures using reflux method, without using additives such as surface reactants. The influence of reaction parameters like temperature and concentration on the growth of nanostructures have been investigated. It has been observed that the nanostructures are formed with a hexagonal nano-plate morphology, grown from a common core. The diameter o...

متن کامل

A high performance lithium-ion battery using LiNa0.02K0.01FePO4/C as cathode material and anatase TiO2 nanotube arrays as anode material

In this paper we report on a lithium ion battery (LIB) based on improved olivine lithium iron phosphate/carbon (LiFePO4/C) as cathode material and LiNa0.02K0.01FePO4/C  synthesized by sol-gel method and TiO2 nanotube arrays (TNAs) with an anatase phasesynthesized through anodization of Ti foil as an anode electrode. Crystallographic structure and surface morphology of the cathode and anode mate...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Atomic layer deposited tungsten nitride thin films as a new lithium-ion battery anode.

This article demonstrates the atomic layer deposition (ALD) of tungsten nitride using tungsten hexacarbonyl [W(CO)6] and ammonia [NH3] and its use as a lithium-ion battery anode. In situ quartz crystal microbalance (QCM), ellipsometry and X-ray reflectivity (XRR) measurements are carried out to confirm the self-limiting behaviour of the deposition. A saturated growth rate of ca. 0.35 Å per ALD ...

متن کامل

Atomic layer deposition of Al2O3 on V2O5 xerogel film for enhanced lithium-ion intercalation stability

V2O5 xerogel films were fabricated by casting V2O5 sols onto fluorine-doped tin oxide glass substrates at room temperature. Five, ten and twenty atomic layers of Al2O3 were grown onto as-fabricated films respectively. The bare film and Al2O3-deposited films all exhibited hydrous V2O5 phase only. Electrochemical impedance spectroscopy study revealed increased surface charge-transfer resistance o...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films

سال: 2017

ISSN: 0734-2101,1520-8559

DOI: 10.1116/1.4987131