Pitting Corrosion in AISI 304 Rolled Stainless Steel Welding at Different Deformation Levels
نویسندگان
چکیده
منابع مشابه
IMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE
Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...
متن کاملSome Studies on Temperature Distribution Modeling of Laser Butt Welding of AISI 304 Stainless Steel Sheets
In this research work, investigations are carried out on Continuous Wave (CW) Nd:YAG laser welding system after preliminary experimentation to understand the influencing parameters associated with laser welding of AISI 304. The experimental procedure involves a series of laser welding trials on AISI 304 stainless steel sheets with various combinations of process parameters like beam power, beam...
متن کاملEnhancement of corrosion protection of AISI 304 stainless steel by nanostructured sol–gel TiO2 films
0010-938X/$ see front matter 2013 Elsevier Ltd. All rights reserved. http://dx.doi.org/10.1016/j.corsci.2013.07.045 ⇑ Corresponding author. Address: Faculty of Mechanical Engineering and Naval Architecture, Departmet of Materials, Ivana Lučića 5, 10000 Zagreb, Croatia. Tel.: +385 1 616 8313; fax: +385 1 615 7126. E-mail address: [email protected] (L. Ćurković). Lidija Ćurković a,⇑, Helena ...
متن کاملFinite Element Simulation of Nd:YAG laser lap welding of AISI 304 Stainless steel sheets
Laser beam welding (LBW) is one of the most important manufacturing processes used for joining of materials. It is also a remarkably complicated, nonlinear operation involving extremely high temperatures. Since its invention more than two decades ago, laser beam welding has been more of an art than a science. Laser welding of austenitic stainless steel AISI 304 the candidate material of this re...
متن کاملMicro abrasion-corrosion of AISI 316L stainless steel
In this study, the synergistic effects of abrasion and corrosion on AISI 316L stainless steel have been investigated using a micro-abrasion test rig. A series of results from abrasioncorrosion tests conducted using the micro-abrasion rig are presented. AISI 316L stainless steel has been studied under both pure abrasion and abrasion-corrosion conditions simulated by either distilled water or 3.5...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Applied Sciences
سال: 2019
ISSN: 2076-3417
DOI: 10.3390/app9163265