Photocorrosion of CdS nanorod arrays and fabrication of CdS@TiO2 core@shell nanorod arrays by atomic layer deposition for improved photostability
نویسندگان
چکیده
منابع مشابه
Fabrication and Characteristics of Self-Aligned ZnO Nanotube and Nanorod Arrays on Si Substrates by Atomic Layer Deposition
Vertically self-aligned ZnO nanorods and nanotubes are fabricated on Si substrates by atomic layer deposition with the assistance of anodic aluminum oxide at 250°C. These nanostructures are equal in height, isolated, and vertical to the Si substrate. With 550 deposition cycles, we can fabricate regular arrays of ZnO nanorods with an average diameter of 70 nm and with a height of 470 nm. In part...
متن کاملTwo-component nanorod arrays by glancing-angle deposition.
A scalable strategy for three-dimensional (3D) assembly of dissimilar materials with nanometer resolution is key to harness the full potential of physical properties expected within the quantum-confined or interface-dominated size regime. Chemical synthesis methods yield layered and coaxial nanowires and branched nanocrystals, while physical vapor deposition (PVD) techniques are particularly ef...
متن کاملGrowth competition during glancing angle deposition of nanorod honeycomb arrays
Arrays of Ta nanorods were grown by glancing angle deposition GLAD onto honeycomb Cr nanodot patterns that were evaporated onto Si substrates through a self-assembled monolayer of SiO2 nanospheres. Statistical size analyses from arrays of rods with variable average length l and width w, with 210 nm l 650 nm and 109 nm w 304 nm, show that the distribution in w broadens with increasing l and decr...
متن کاملInvestigating structural, optical and photocatalytic properties of hydrothermally synthesized ZnO nanorod arrays with various aspect ratios
ZnO nanorods with various aspect ratios (by changing the time of growth between 0-240 min) were synthesized using hydrothermal method and were investigated using XRD, SEM, UV–Vis and PL. It was found that growth time is directly coupled with the length, orientation and aspect ratio of the nanorod arrays. The optical transmittance of the NR arrays indicated a regular decrement of average transmi...
متن کاملFast UV detection by Cu-doped ZnO nanorod arrays chemically deposited on PET substrate
Well-aligned Cu-doped ZnO nanorods were successfully synthesized on polyethylene terephthalate (PET) substrate using chemical bath deposition method. The structural and optical properties of Cu-doped ZnO nanorods were investigated using X-ray diffraction (XRD), field-emission scanning electron microscopy (FESEM), energy dispersive X-ray spectroscopy (EDX) and photoluminescence (PL) spectroscopy...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Optical Materials: X
سال: 2021
ISSN: 2590-1478
DOI: 10.1016/j.omx.2021.100070