Photocatalytic Properties of Co3O4-Coated TiO2 Powders Prepared by Plasma-Enhanced Atomic Layer Deposition

Co3O4-coated commercial TiO2 powders (P25) p-n junction photocatalysts were prepared by plasma-enhanced atomic layer deposition (PEALD) technique. The structure, morphology, bandgap, and photocatalytic properties under ultraviolet light were investigated systematically. Although the deposition of Co3O4 does not change the anatase structure and crystallite size of P25 powders, the ultraviolet ph...

متن کامل

Antioxidation properties of Ti0.83Al0.17N prepared using plasma-enhanced atomic layer deposition

The high-temperature antioxidation behavior of Ti0.83Al0.17N prepared using plasma-enhanced atomic layer deposition sPEALDd with TiCl4, AlCl3, N2/H2/Ar, and NH3/H2/Ar radicals were studied. One cycle for depositing Ti0.83Al0.17N consisted of eight TiN cycles followed by two AlN cycles. After forming a 30-nm-thick Ti0.83Al0.17N film, the film was oxidized in ambient O2 at 650 °C for 30 min. The ...

متن کامل

Optical and microstructural properties of ZnO/TiO2 nanolaminates prepared by atomic layer deposition

ZnO/TiO2 nanolaminates were grown on Si (100) and quartz substrates by atomic layer deposition at 200°C using diethylzinc, titanium isopropoxide, and deionized water as precursors. All prepared multilayers are nominally 50 nm thick with a varying number of alternating TiO2 and ZnO layers. Sample thickness and ellipsometric spectra were measured using a spectroscopic ellipsometer, and the parame...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Microscopic Study of Atomic Layer Deposition of TiO2 on GaAs and Its Photocatalytic Application

We report a microscopic study of p-GaAs/TiO2 heterojunctions using cross-sectional high resolution transmission electron microscopy (HRTEM). The photocatalytic performance for both H2 evolution and CO2 reduction of these heterostructures shows a very strong dependence on the thickness of the TiO2 over the range of 0−15 nm. Thinner films (1−10 nm) are amorphous and show enhanced catalytic perfor...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nanoscale Research Letters

سال: 2017

ISSN: 1931-7573,1556-276X

DOI: 10.1186/s11671-017-2269-4