We here demonstrate a new route for deposition of phosphorous based materials by atomic layer (ALD) using the phosphites Me3PO3 or Et3PO3 as precursors. These contain in oxidation state (III) and are open reduced phases ALD. have investigated their applicability synthesis LiPO AlPO characterized growth means situ quartz crystal microbalance. Phosphites good alternatives to established phosphate-based routes they high vapor pressure compatible with water coreactant during deposition. The deposited been XPS, x-ray fluorescence, ion beam analysis composition analysis, spectroscopic ellipsometry thickness, FTIR local structure.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic layer deposition (ALD): from precursors to thin film structures

The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...

متن کامل

Thin, high atomic weight refractory film deposition for diffusion barrier, adhesion layer, and seed layer applications

Related Articles The Si3N4/TiN Interface: 4. Si3N4/TiN(001) Grown with a −250 V Substrate Bias and Analyzed In situ using Angle-resolved X-ray Photoelectron Spectroscopy Surf. Sci. Spectra 19, 62 (2012) The Si3N4/TiN Interface: 1. TiN(001) Grown and Analyzed In situ using Angle-resolved X-ray Photoelectron Spectroscopy Surf. Sci. Spectra 19, 33 (2012) The Si3N4/TiN Interface: 5. TiN/Si3N4 Grown...

متن کامل

Bi-layer Channel AZO/ZnO Thin Film Transistors Fabricated by Atomic Layer Deposition Technique

This letter demonstrates bi-layer channel Al-doped ZnO/ZnO thin film transistors (AZO/ZnO TFTs) via atomic layer deposition process at a relatively low temperature. The effects of annealing in oxygen atmosphere at different temperatures have also been investigated. The ALD bi-layer channel AZO/ZnO TFTs annealed in dry O2 at 300 °C exhibit a low leakage current of 2.5 × 10-13A, I on/I off ratio ...

متن کامل

Thermo-Optical Properties of Thin-Film TiO2–Al2O3 Bilayers Fabricated by Atomic Layer Deposition

We investigate the optical and thermo-optical properties of amorphous TiO2–Al2O3 thin-film bilayers fabricated by atomic layer deposition (ALD). Seven samples of TiO2–Al2O3 bilayers are fabricated by growing Al2O3 films of different thicknesses on the surface of TiO2 films of constant thickness (100 nm). Temperature-induced changes in the optical refractive indices of these thin-film bilayers a...

متن کامل

Film growth model of atomic layer deposition for multicomponent thin films

Atomic layer deposition sALDd has become an essential technique for fabricating nano-scale thin films in the microelectronics industry, and its applications have been extended to multicomponent thin films, as well as to single metal oxide and nitride films. A mathematical film growth model for ALD is proposed to predict the deposition characteristics of multicomponent thin films grown mainly in...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of vacuum science & technology

سال: 2021

ISSN: ['2327-9877', '0734-211X']

DOI: https://doi.org/10.1116/6.0000844