Phase discrimination between ? and ? phases in the new nickel-based superalloy VDM Alloy 780 using EBSD

نویسندگان

چکیده

VDM Alloy 780 is a new nickel-based superalloy developed for higher service temperatures up to 750 °C. In addition fine ??-Ni3(Al,Ti) strengthening precipitates, grain boundary precipitates resembling ?-Ni3Nb and/or ?-Ni3Ti phases are also observed in this alloy. Previous studies on 718Plus, with chemical composition close 780, revealed that phase discrimination between ? and ? particles not straightforward requires the use of high-resolution characterization techniques such as HRTEM. This work aims at evaluating EBSD technique regards identification these plate-shaped particles. Classical indexing diffraction patterns based Kikuchi band detection Hough space fails differentiate two phases. However approaches comparison experimental simulated patterns, least partly, could overcome issue. The advanced dictionary-based approach involves simulation dynamic electron scattering events identified main component consistent recently published HRTEM investigation 780. Refinement classical method under kinematic assumptions implemented “Refined Accuracy” mode Oxford AZtec software package led appreciable improvement.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

the relationship between learners critical thinking ability and their performance in the reading sections of the tofel and ielts test

the study reflected in this thesis aims at finding out relationships between critical thinking (ct), and the reading sections of tofel and ielts tests. the study tries to find any relationships between the ct ability of students and their performance on reading tests of tofel and academic ielts. however, no research has ever been conducted to investigate the relationship between ct and the read...

15 صفحه اول

on the relationship between using discourse markers and the quality of expository and argumentative academic writing of iranian english majors

the aim of the present study was to investigate the frequency and the type of discourse markers used in the argumentative and expository writings of iranian efl learners and the differences between these text features in the two essay genres. the study also aimed at examining the influence of the use of discourse markers on the participants’ writing quality. to this end the discourse markers us...

15 صفحه اول

A new dental superalloy system. I. Theory and alloy design.

Basic factors that influence the physical metallurgy and the mechanical properties of cobalt-base alloys are discussed in this study; these factors include the coherency of the interphase interface, the stacking fault energy, and the average electron hole number. Control of these factors and considerations of corrosion resistance and body compatibility determined the compositions for alloys tha...

متن کامل

Recent Advances in Creep Modelling of the Nickel Base Superalloy, Alloy 720Li

Recent work in the creep field has indicated that the traditional methodologies involving power law equations are not sufficient to describe wide ranging creep behaviour. More recent approaches such as the Wilshire equations however, have shown promise in a wide range of materials, particularly in extrapolation of short term results to long term predictions. In the aerospace industry however, l...

متن کامل

Automatic evaluation of nickel alloy secondary phases from SEM images.

Quantitative metallography is a technique to determine and correlate the microstructures of materials with their properties and behavior. Generic commercial image processing and analysis software packages have been used to quantify material phases from metallographic images. However, these all-purpose solutions also have some drawbacks, particularly when applied to segmentation of material phas...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Characterization

سال: 2021

ISSN: ['1044-5803', '1873-4189']

DOI: https://doi.org/10.1016/j.matchar.2021.111105