Parameters Affecting Bulk Etch Rate VBfor CR-39 Detector

نویسندگان

چکیده

In this work, the dependence of bulk etches rate VB for CR-39detector on thetemperature T, etching time t and concentration N NaOH etchant solution has been studied fordetectors material types PADC. The concentration, time, temperatureand other conditions havebeen varied in ranges (5.25-8.25) N, (1-5) hand (60-80) °C PADC respectively. case, thickness removed by from 0.20 to 6.10

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

E ects of stirring on the bulk etch rate of CR-39 detector

It is well established that the bulk etch rates for solid state nuclear track detectors are a ected by the concentration and the temperature of the etchant. Recently, we found that the bulk etch rate for the LR 115 detector to be a ected by stirring during etching. In the present work, the e ects of stirring on the bulk etch rate of the CR-39 detector is investigated. One set of sample was etch...

متن کامل

Bulk and track etch properties of CR-39 SSNTD etched in NaOH/ethanol

Recently, Matiullah et al. described the use of NaOH/ethanol as an etchant for the CR-39 detector, and have determined the corresponding bulk and track etch properties from the track diameter method. In the present work, the bulk and track etch properties of CR39 in NaOH/ethanol were derived from direct measurements. The bulk etch rate has been found to increase with the molarity of NaOH/ ethan...

متن کامل

Proton beam dosimetry by CR-39 track-etched detector

Background: High and intermediate energy protons are not able to form a track in a solid state nuclear track detector (SSNTD) directly. However, such tracks can be formed through secondary particles created during primary radiation nuclear reactions in a SSNTD. Materials and Methods: The protons with primary energies of 9.6 and 30 MeV available at the cyclotron accelerator with corresponding lo...

متن کامل

Measurement of parameters of tracks in CR-39 detector from replicas.

In determining the etched track rate in solid-state nuclear track detectors, track lengths should be determined accurately. A method based on surface profilometry is proposed to determine the track lengths in CR-39 detectors through measurements of their replicas. Tracks from alpha particles with an incident energy of 4 MeV have been chosen to demonstrate the method. After irradiation and chemi...

متن کامل

E ects of stirring on the bulk etch rate of LR 115 detector

The e ects of stirring on the bulk etch rate of LR 115 detector has been investigated. The surface pro6le measurement method using an instrument called Form Talysurf has been used to measure the thickness of the active layer of the LR 115 detectors. The etchant was 10% aqueous solution of NaOH maintained at 60◦C. The bulk etch rate under magnetic stirring has been found to be 6:65 ± 0:34 m h−1 ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Ma?alla? ??mi?a? al-anb?r li-l-?ul?m al-?irfa?

سال: 2022

ISSN: ['1991-8941', '2706-6703']

DOI: https://doi.org/10.37652/juaps.2022.172390