Panel tests for thermal spalling of fire-clay bricks used at high temperatures
نویسندگان
چکیده
منابع مشابه
Thermal Degradation of Polymers at High Temperatures
Work on thermal ~egradation of poly mers has prev iously been carried out aL lempC'mt ures up to about 500 G. In the present work the range has been extend cd to 850 0 C. Polystyrene was pyrolyzed in a vacuum and also in helium at atmos pheric pressure at 3620 and at 850 0 C. Analysis of t he volatile products indicates that higher temperatures a nd hi~her. pressures cause a greater fragmen tat...
متن کاملThermal behavior of ethylene/1-octene copolymer fractions at high temperatures: Effect of hexyl branch content
In this work, the effect of hexyl branch content on thermal behavior of a fractionated ethylene/1-octene copolymer with emphasis on high temperatures was investigated. The ethylene/1-octene copolymer was carefully fractionated to different fractions with homogenous hexyl branch (HB) content by preparative temperature rising elution fractionation (P-TREF) method. The P-TREF fractions were therma...
متن کاملResidual Mechanical Properties of Concrete Made with Crushed Clay Bricks and Roof Tiles Aggregate after Exposure to High Temperatures
This paper presents the residual mechanical properties of concrete made with crushed bricks and clay roof tile aggregates after exposure to high temperatures. One referent mixture and eight mixtures with different percentages of replacement of natural aggregate by crushed bricks and roof tiles are experimentally tested. The properties of the concrete were measured before and after exposure to 2...
متن کاملThermal properties of iron at high pressures and temperatures.
We investigate the thermoelastic properties of close-packed phases of iron at pressures up to 400 GPa and temperature to 6000 K using a tight-binding total-energy method and the cell model of the vibrational partition function. The calculated properties are in good agreement with available static and shock-wave experimental measurements. The compressional behavior of a number of thermoelastic p...
متن کاملDensity, Strength, Thermal Conductivity and Leachate Characteristics of Light-Weight Fired Clay Bricks Incorporating Cigarette Butts
Several trillion cigarettes produced worldwide annually lead to many thousands of kilograms of toxic waste. Cigarette butts (CBs) accumulate in the environment due to the poor biodegradability of the cellulose acetate filters. This paper presents some of the results from a continuing study on recycling CBs into fired clay bricks. Physico-mechanical properties of fired clay bricks manufactured w...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Research of the National Bureau of Standards
سال: 1945
ISSN: 0091-0635
DOI: 10.6028/jres.034.035