Optimization of Micro-arc Oxidation Parameters for Preparing AlN Complex Ceramic Coatings on 1060 Al Substrate

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

n-SiO2 Embedded HA/TiO2 Composite Coatings Deposited on Pure Titanium Substrate by Micro-Arc Oxidation

As orthopaedic and dental metallic implant materials, titanium and titanium alloys are widely used due to their relatively low modulus, good fracture toughness, excellent strenthto-weight ration, and superior biocompatibility and corrosion resistance (Long and Rack, 1998). They have become the first choice above all other candidate metallic implant materials such as Co-Cr-Mo alloys, stainless s...

متن کامل

Influence of KMnO4 Concentrationon Infrared Emissivity of Coatings Formed on TC4 Alloys by Micro-Arc Oxidation

Ceramic coatings with high emissivity were fabricated on TC4 alloys by micro-arc oxidation technique (MAO) in mixed silicate and phosphate electrolytes with varying KMnO₄ addition. The microstructure, phase and chemical composition were characterized by scanning electron microscope (SEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS), and the infrared emissivity of the MAO...

متن کامل

Oxidation behavior of AlN/CrN multilayered hard coatings

We report on the oxidation behavior of AlN/CrN multilayers at 900 °C, deposited by radio frequency magnetron sputtering. It is shown that oxidation in this system is controlled by diffusion of Cr towards the surface and formation of Cr2O3. Cr diffusion is found to mainly occur along grain boundaries. Thus, coherent cubic AlN/CrN multilayer regions with coarse columnar grain structures are found...

متن کامل

Phlogopite glass-ceramic coatings on stainless steel substrate by plasma spray

Macor coatings on 316 alloys substrates were prepared by plasma spraying. The crystallization temperature, thermal expansion coefficient of mica glass-ceramic were at 900ºC and 40× 10−7/◦C respectively. The microhardness of obtained glass-ceramic coating was 6.8GPa and the coefficient friction was 0.98 . 

متن کامل

Investigation of Zinc and Phosphorus Elements Incorporated into Micro-Arc Oxidation Coatings Developed on Ti-6Al-4V Alloys

In order to clarify the mechanism that zinc and phosphorus elements entering the micro-arc oxidation (MAO) coatings developed on Ti-6Al-4V alloys, anodic coatings containing different zinc and phosphorus were fabricated using an orthogonal experiment of four factors with three levels in an electrolyte containing EDTA-ZnNa₂, KOH, and phytic acid. Surface morphology, element composition, chemical...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Physics: Conference Series

سال: 2021

ISSN: 1742-6588,1742-6596

DOI: 10.1088/1742-6596/1732/1/012122