Wear and Mechanical Properties of Nodular Iron Modified with Copper
In this research (using induction furnace process) nodular iron with three different percentages of copper (residual, 0.5% and 1,2%) was obtained. Chemical analysis was performed by mass spectrometry and microstructures were characterized by Optical Microscopy (ASTM E3) and Scanning Electron Microscopy (SEM). The study of mechanical behavior was carried out in a mechanical test machine (ASTM E8...
متن کاملLiterature search - Deteriorated Graphite Structures on Cast Iron Skins
The fatigue strength offerritic ductile iron, Grade EN-GJS-400-18U-LT. was determined for large section castings measuring 4 by 24 by 24 inches. Fatigue testing was conducted in bending fatigue in order to determine the influence of surface conditions on fatigue strength. Test specimens with various surface conditions were evaluated, including notched and un-notched specimens, as well as those ...
متن کاملAuto-analysis system for graphite morphology of grey cast iron
The current method to classify graphite morphology types of grey cast iron is based on traditional subjective observation, and it cannot be used for quantitative analysis. Since microstructures have a great effect on the mechanical properties of grey cast iron and different types have totally different characters, six types of grey cast iron are discussed and an image-processing software subsys...
متن کاملenvironmental effects of gol-e-gohar iron ore mine on groundwater of the area
gol-e-gohar iron ore mine of sirjan in southern part of iran is a large open pit that operates below the groundwater table and during mining operation, dewatering is required to prevent operation processes from flooding. current operation is going on by digging wells in or out of the pit and pumping to prevent flooding. as a result of the former dewatering operation a vast deep cone of depressi...
Failure Analysis of a Four Cylinder Diesel Engine Crankshaft Made From Nodular Cast Iron
The premature breakage in some four cylinder diesel engine crankshafts was reported. All crankshafts were failed from the same region. Failures had occurred in the first crankpin, the nearest crankpin to the flywheel. Dynamic analysis and finite element modelling were carried out to determine the state of stress in the crankshaft. FEM results revealed that the first crankpin fillet is the most ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Society of Precision Engineering
سال: 1951
ISSN: 0374-3543
DOI: 10.2493/jjspe1933.17.367