On the Temper Hardening Properties of Cobalt-Tungsten Alloys
نویسندگان
چکیده
منابع مشابه
Mechanical Properties of Electroformed Nickel Cobalt Alloys
Mechanical properties of nickel-cobalt alloys (0-10% Co) electroformed with low internal stress in sulfamate-based solutions were investigated in as deposited and heat treated conditions. It was demonstrated that alloy properties can be modified by selecting deposition conditions and alloy composition. Recommendations on alloy selection are made based on application requirements. The higher str...
متن کاملcontrol of the optical properties of nanoparticles by laser fields
در این پایان نامه، درهمتنیدگی بین یک سیستم نقطه کوانتومی دوگانه(مولکول نقطه کوانتومی) و میدان مورد مطالعه قرار گرفته است. از آنتروپی ون نیومن به عنوان ابزاری برای بررسی درهمتنیدگی بین اتم و میدان استفاده شده و تاثیر پارامترهای مختلف، نظیر تونل زنی(که توسط تغییر ولتاژ ایجاد می شود)، شدت میدان و نسبت دو گسیل خودبخودی بر رفتار درجه درهمتنیدگی سیستم بررسی شده اشت.با تغییر هر یک از این پارامترها، در...
15 صفحه اولPrecipitation Hardening of Metal Alloys
Precipitation hardening, or age hardening, provides one of the most widely used mechanisms for the strengthening of metal alloys. The fundamental understanding and basis for this technique was established in early work at the U. S. Bureau of Standards on an alloy known as Duralumin [1,2]. Duralumin is an aluminum alloy containing copper and magnesium with small amounts of iron and silicon. In a...
متن کاملCobalt with tungsten carbide
in the testicular damage caused by indium arsenide and indium phosphide in hamsters during two years after intratracheal instillations. (CIGS) nanocrystal " inks " for printable photovoltaics. Selective sequential dissolution for the determination of inorganic indium compounds in the particulate matter of emissions and workplace air. Current evaluation Conclusion from the previous Monograph (IA...
متن کاملSURFACE HARDENING OF TUNGSTEN-BASED HEAVY ALLOY VIA PACK BORONIZING
The boronizing of a tungsten heavy alloy containing Ni and Fe as the major alloying elements were performed in the present study to increase its surface hardening. Pack cementation method was employed as a well-known, successful solid-state process for boronizing. The coating treatment was accomplished at different temperatures of 1000, 1050 and 1100°C for 6 and 9 hours. The formation of tu...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Transactions of the Japan Institute of Metals
سال: 1965
ISSN: 0021-4434,2432-4701
DOI: 10.2320/matertrans1960.6.139