On the Study of Thermal Transitions in Selected n-Paraffins Using Differential Scanning Calorimetry

نویسندگان

چکیده

The results obtained from a study of the thermal transformations polymorphic long-chain normal paraffins (n-C32H66 and n-C36H74) are presented here. research was performed using power-compensated Differential Scanning Calorimeter (DSC). Both heating cooling experiments were in dynamic nitrogen atmosphere. Thermodynamic data for both transitions, as well fusion endotherms, determined DSC curves. Using heats transition (?H), Joules/gram, curves, molar kJ/mol, calculated compared to previously published values. entropy (?S) then each observed events. Additional information is given by author on obtaining best use behavior n-paraffins. This manuscript opens with review most early work it provided dealing polymorphism n-paraffin solids. Some this referenced prior advent computerized analytical instrumentation.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Surveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by Differential Scanning Calorimetry (DSC)

One of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. In this paper, the authors have studied thermal behaviour for Schiff base ligand and their synthesized Cobalt, Nickel complexes. In this method, the sample is opposed to a controlled temperature change and its physical properties. Here we studied melting point and Tg...

متن کامل

Surveying the effects of silver nanoparticle on thermal properties of some calyx [4]arene compounds by Differential Scanning Calorimetry (DSC)

One of the best and the most active ways for surveying thermal behaviour of materials is using differential scanning calorimetry. In this paper, the authors have studied thermal behaviour for Schiff base ligand and their synthesized Cobalt, Nickel complexes. In this method, the sample is opposed to a controlled temperature change and its physical properties. Here we studied melting point and Tg...

متن کامل

Study of the thermal behavior of azidohetarenes with differential scanning calorimetry.

Thermal properties of azidohetarenes without reactive ortho-substituents, obtained by DSC analysis, were compared with the DSC data of ortho-phenyl and ortho-acyl substituted azidohetarenes, which give ring closure reactions either to indoles or to five-membered heterocycles such as isoxazoles. The reaction temperatures and reaction enthalpies give both information to prepare the reaction condi...

متن کامل

Differential scanning calorimetry of bacteria.

Thermograms obtained by differential scanning calorimetry of a range of bacteria of different heat resistances were compared. Equations were derived to calculate the rate at which the numbers of viable organisms in a calorimeter decline as the temperature is raised at a constant rate. Vegetative bacteria scanned at 10 degrees C min-1 showed multi-peaked thermograms with four major peaks (denote...

متن کامل

Differential Scanning Calorimetry of Whole

Cereal Chem. 66(4):317-320 The thermal properties of whole grain milled rice and milled rice flour samples. Gelatinization enthalpies were about 40% greater in whole grain were investigated by differential scanning calorimetry. Thermal curves rice compared to rice flour for each variety. Heating rate studies conducted were obtained on representative long, medium, short, and very low amylose on ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Thermo

سال: 2022

ISSN: ['2673-7264']

DOI: https://doi.org/10.3390/thermo2030021