On the Recrystallization Behavior at Weld Heat-affected-zone of Commercially pure Aluminum
نویسندگان
چکیده
منابع مشابه
Investigation on the Deformation Behavior and Strain Distribution of Commercially Pure Aluminum after Circular Simple Shear Extrusion
Circular simple shear extrusion process was introduced as a new geometry for simple shear extrusion technique to fabricate ultrafine-grained materials. Similar to the simple shear extrusion method, this process is also based on direct extrusion, and the samples deform in a simple shear manner. In this investigation, the simulations were carried out using the commercial finite element code ABAQU...
متن کاملFatigue and Fracture Behavior of a Cold-Drawn Commercially Pure Aluminum Wire
Fatigue properties and cracking behavior of cold-drawn commercially pure aluminum wires (CPAWs) widely used as the overhead transmission conductors were investigated. It was found that the fracture surface of the CPAWs shows an obvious four-stage fracture characteristic, i.e., crack initiation, planar crack propagation, 45°-inclined crack propagation and final rapid fracture. The crack growth m...
متن کاملتاثیر تعمیر مکرر بر ریزساختار، خواص مکانیکی و رفتار خوردگی مقاطع جوشکاری شده آلیاژ آلومینیم 321H-5083 به روش میگ پالسی
In the marine industries, defects in welded joints are repaired to improve the performance. It is possible that a welded joint is repaired once or twice. In this research, effect of repair on microstructure, mechanical properties and corrosion behavior of welded joints of 5083-H321 aluminum alloy using pulsed MIG process was investigated. The results show that excess heat due to increasing the ...
متن کاملThe Influence of Silicon Content on Recrystallization of Twin-Roll Cast Aluminum Alloys for Heat Exchangers
متن کامل
Friction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium
In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Welding Society
سال: 1974
ISSN: 0021-4787,1883-7204
DOI: 10.2207/qjjws1943.43.274