On the Pitting Corrosion Resistance of Titanium

نویسندگان
چکیده

منابع مشابه

Effect of Long-term Immersion on the Pitting Corrosion Resistance of Nitinol

One of the challenges faced by medical-device manufacturers is the use of short-term in-vitro data to evaluate the long-term in-vivo corrosion performance of implants. In this study, mechanically polished Nitinol wires were immersed in phosphate-buffered saline (PBS) at 37 °C for up to one week prior to performing cyclic polarization tests. Results are presented that show the effect of immersio...

متن کامل

INVESTIGATION ON THE EFFECTS OF MAGNETIC FIELD ON BROMIDE-INDUCED PITTING OF COMMERCIALLY PURE TITANIUM

Abstract: In chloride salt solutions, titanium alloys exhibit reasonably high pitting potentials as high as +10 V (vs. Ag/AgCl) at room temperatures. On the other hand, anodic pitting potentials are significantly lower in bromide solutions. In this study, pitting corrosion of commercially pure titanium in aqueous NaBr solution of 0.1 M concentration at room temperature was studied and the e...

متن کامل

Effect of Deformation-Induced Defects on the Microstructure and Pitting Corrosion Behavior of Al-Ag Alloy

In this study, a wide range of combined ageing treatments and cold work deformations in the Al 4.2 wt% Ag alloy matrix were proposed, aiming to investigate the effect of defects such as precipitates (Ag2Al plates) and dislocations on the mechanical and electrochemical behavior of Al–4.2 wt% Ag alloys. Further reductions of thickness from 10 to 60%, decreases the mean size of Ag2...

متن کامل

Atomic-scale decoration for improving the pitting corrosion resistance of austenitic stainless steels

Stainless steels are susceptible to the localized pitting corrosion that leads to a huge loss to our society. Studies in the past decades confirmed that the pitting events generally originate from the local dissolution in MnS inclusions which are more or less ubiquitous in stainless steels. Although a recent study indicated that endogenous MnCr2O4 nano-octahedra within the MnS medium give rise ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: CORROSION ENGINEERING DIGEST

سال: 1959

ISSN: 0010-9355,1884-1155

DOI: 10.3323/jcorr1954.8.8_327