On pressed plate of copper-aluminium friction welded joint.

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Friction Stir Welded 2024-T351 Aluminium Alloy

Fatigue failure characteristics of friction stir welds in 13mm gauge 2024-T351 plate have been assessed. Failure occurred from either the weld region (nugget/flow arm) or from the material immediately surrounding the weld. Fatigue failure from the surrounding material was essentially conventional, initiating from large S-phase intermetallic particles and growing in a macroscopic mode I manner. ...

متن کامل

The Strength of Friction Stir Welded and Friction Stir Processed Aluminium Alloys

Local strength of friction stir (FS) welds and FS processed aluminium alloys in heat treatable aluminium alloys is dominated by precipitation hardening. Strengthening due to stored dislocations is generally limited to 40MPa, and grain size strengthening is generally less than 10MPa. Local crystallographic texture can cause yield strength variation on the order of 5%. Published models for streng...

متن کامل

Effect of tool position on microstructural and mechanical properties of friction stir butt welded joint of AA2024–AA7075 dissimilar alloys

In this research, butt joining of Al2024 and Al7075 plates were performed by Friction Stir Welding (FSW) and the effect of tool position on microstructural and mechanical properties in about 1 mm from center line of joint towards the advancing side (AS) and the retreating side (RS) was investigated at three positions of +1, 0, -1 mm. In this regard, the plates of Al2024 and Al7075 were selected...

متن کامل

Evaluation of microstructure and mechanical properties of friction stir welded copper / 316L stainless steel dissimilar metals

In the present research, friction stir welding (FSW) process was used for butt joining of pure copper plate to 316L stainless steel plate. Mechanical properties and microstructural characteristics of the joint were evaluated by microhardness and tensile tests as well as optical and scanning electron microscope (SEM). It was found that microstructure of the weld nugget (WN) has fine grains where...

متن کامل

Microstructure and Mechanical Properties of the Friction Welded Joint between X53CrMnNiN219 and X45CrSi93 Stainless Steel

Dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. In this study, X53CrMnNiN219 (austenitic stainless steel) and X45CrSi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. The welded joint was then heat treated at 760 0C for 60 min. Mechanical prop...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY

سال: 1986

ISSN: 0288-4771

DOI: 10.2207/qjjws.4.697