Notched Tensile Strength and Fatigue Crack Growth Behavior of Ti-6Al-6V-2Sn Laser Welds

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

EFFECTS OF TENSILE STRENGTH ON FATIGUE BEHAVIOR AND NOTCH SENSITIVITY OF TI-6AL-4V

In this research, rotating bending fatigue test at minimum to maximum stress ratio of R=-1 was used for investigating the fatigue behavior of Ti-6Al-4V alloy. Both smooth and notched specimens, with elastic concentration factor, kt, of approximately 3.6 and 4.1 were used for this purpose.In addition, the effect of variation in ultimate tensile strength, UTS, on the fatigue behavior of this allo...

متن کامل

Mixed-Mode, High-Cycle Fatigue-Crack Growth Thresholds in Ti-6Al-4V: A Comparison of Large and Small Crack Behavior

There are few experimental results to date describing the crack-propagation threshold behavior of short fatigue cracks under multiaxial loading conditions. To address this need, in the present study, the variation in mixed-mode, high-cycle fatigue-crack growth thresholds with crack size and shape are reported for a Ti-6Al-4V turbine blade alloy, heat treated to two widely different microstructu...

متن کامل

Tensile and fatigue strength of hydrogen-treated Ti-6Al-4V alloy

Tensile, fatigue and fractographic data on Ti-6AI-4V microstructures attained through a series of post-L3-annealing treatments which used hydrogen as a temporary alloying element are presented. Hydrogen-alloying treatments break up the continuous grain boundary 0c and colony structure, and produce a homogeneous microstructure consisting of refined s-grains in a matrix of discontinuous 13. These...

متن کامل

Hot Deformation Behavior of Ti-3.5Al-5Mo-6V-3Cr-2Sn-0.5Fe Alloy in α + β Field

The deformation behavior of Ti-3.5Al-5Mo-6V-3Cr-2Sn-0.5Fe high strength β titanium alloy is systematically investigated by isothermal compression in α + β field with the deformation temperatures ranging from 1003 K to 1078 K, the strain rates ranging from 0.001 s to 1 s and the height reduction is around 50%. Essentially, the flow stress-strain curve of isothermal compression in α + β field exh...

متن کامل

Mixed-mode, high-cycle fatigue-crack growth thresholds in Ti– 6Al–4V: Role of small cracks

There have been few studies to date describing fatigue-crack propagation thresholds under mixed-mode loading conditions in the presence of cracks, that are small as compared to the characteristic microstructural dimensions. To address this need, the variation in mixed-mode, high-cycle fatigue-crack growth thresholds with crack size is reported for a Ti-6Al-4V turbine blade alloy with a fine-gra...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MATERIALS TRANSACTIONS

سال: 2009

ISSN: 1345-9678,1347-5320

DOI: 10.2320/matertrans.m2009001