New Inexpensive Simple Experimental Setup for Anodic Bonding of Silicon-Glass

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Study on the Glass Silicon Anodic Direct Bonding Parameters

By MEMS packaging test platform for bonding process of bonding temperature and bonding time, and test silicon specifications experimental study. Experimental results indicate that when the bonding voltage of 1200V, bonding temperature of 445 0 C to 455 0 C, bonding time is 60s, the void fraction is less than 5%. Glass and silicon wafer bonding quality can achieve the best. The experimental resu...

متن کامل

A Microsystem Based on Porous Silicon-Glass Anodic Bonding for Gas and Liquid Optical Sensing

We have recently presented an integrated silicon-glass opto-chemical sensor for lab-on-chip applications, based on porous silicon and anodic bonding technologies. In this work, we have optically characterized the sensor response on exposure to vapors of several organic compounds by means of reflectivity measurements. The interaction between the porous silicon, which acts as transducer layer, an...

متن کامل

Examination of Glass-Silicon and Glass-Glass Bonding Techniques for Microfluidic Systems

We report here on the results of experiments concerning particular bonding processes potentially useful for ultimate miniaturization of microfluidic systems. Direct anodic bonding of continuous thin Pyrex glass of 250 pm thickness to silicon substrates gives multiple, large voids in the glass. Etchback of thick glass of 1200 pm thickness bonded to silicon substrates gives thin continuous glass ...

متن کامل

A Hermetic Glass–Silicon Package Formed Using Localized Aluminum/Silicon–Glass Bonding

A hermetic package based on localized aluminum/silicon-to-glass bonding has been successfully demonstrated. Less than 0.2 MPa contact pressure with 46 mA current input for two parallel 3.5m-wide polysilicon on-chip microheaters can raise the temperature of the bonding region to 700 C bonding temperature and achieve a strong and reliable bond in 7.5 min. The formation of aluminum oxide with sili...

متن کامل

Transmission Laser Bonding of Glass with Silicon Wafer

As a microassembly and an encapsulation technique, wafer bonding offers a unique opportunity to combine different materials. Transmission laser bonding not only can satisfy wafer level bonding requirements, but can also be directly implemented into the existing automatic semiconductor fabrication line. In this paper, a laser-induced wafer bonding technique for micro-electro-mechanical systems (...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: ECS Journal of Solid State Science and Technology

سال: 2021

ISSN: 2162-8769,2162-8777

DOI: 10.1149/2162-8777/abfb0e