Nanoindentation strain-rate jump tests for determining the local strain-rate sensitivity in nanocrystalline Ni and ultrafine-grained Al

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Texture dependent strain rate sensitivity of ultrafine-grained aluminum films

Article history: Received 25 October 2015 Received in revised form 2 December 2015 Accepted 3 December 2015 Available online 17 December 2015 We investigated the strain rate sensitivity (SRS) of freestanding ultrafine-grained aluminum films with similar thickness (~240 nm) and mean grain size (~275 nm) but highly dissimilar texture. For (110) textured bicrystalline films, flow stress increased ...

متن کامل

High-strain-rate nanoindentation behavior of fine-grained magnesium alloys

rate nanoindentation behavior of fine-grained magnesium alloys. " Article is made available in accordance with the publisher's policy and may be subject to US copyright law. Please refer to the publisher's site for terms of use. The MIT Faculty has made this article openly available. Please share how this access benefits you. Your story matters. The effects of temperature and alloying elements ...

متن کامل

Strain-rate dependence for Ni/Al hybrid foams

Shock absorption often needs stiff but lightweight materials that exhibit a large kinetic energy absorption capability. Open-cell metal foams are artificial structures, which due to their plateau stress, including a strong hysteresis, can in principle absorb large amounts of energy. However, their plateau stress is too low for many applications. In this study, we use highly novel and promising ...

متن کامل

Strain Rate Sensitivity Studies of Cryomilled Al Alloy Performed by Nanoindentation

Al 5083 alloy powder was mechanically milled in liquid nitrogen to achieve a nanocrystalline (NC) structure having an average grain size of 50 nm with high thermal stability, and then consolidated by quasi-isostatic (QI) forging. The consolidation resulted in ultrafine grains (UFG) of about 250 nm, and the bulk material exhibited enhanced strength compared to conventionally processed Al 5083. T...

متن کامل

Strain rate sensitivity of nanocrystalline Au films at room temperature

The effect of strain rate on the inelastic properties of nanocrystalline Au films was quantified with 0.85 and 1.76 lm free-standing microscale tension specimens tested over eight decades of strain rate, between 6 10 6 and 20 s . The elastic modulus was independent of the strain rate, 66 ± 4.5 GPa, but the inelastic mechanical response was clearly rate sensitive. The yield strength and the ulti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Research

سال: 2011

ISSN: 0884-2914,2044-5326

DOI: 10.1557/jmr.2011.156