Nanoindentation on peeled high-performance polymeric fibers reveals failure mechanisms

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A FEM Multiscale Homogenization Procedure using Nanoindentation for High Performance Concrete

This paper aims to develop a numerical multiscale homogenization method for prediction of elasto-viscoplastic properties of a high performance concrete (HPC). The homogenization procedure is separated into two-levels according to the microstructure of the HPC: the mortar or matrix level and the concrete level. The elasto-viscoplastic behavior of individual microstructural phases of the matrix a...

متن کامل

Rapid Solidification of Polymeric Fibers

A thorough understanding of crystallization kinetics for rapid polymer solidification during the fiber spinning process is a route to maximizing fiber properties while increasing production speeds. We are using theoretical, computational, and experimental models to characterize the crystallization process at the molecular, microscopic, and macroscopic levels. Polymer dependent molecular descrip...

متن کامل

Fracture Failure Mechanisms of Long Single PA6 Fibers

The present study investigates the failure mechanisms of industrial fiber materials, using a custom designed fiber cutting performance test bench. The fracture morphologies of single PA6 fibers are examined by scanning electron microscopy. The analysis reveals that fiber cutting can be distinguished according to four distinct stages of fiber failure represented by shearing, cutting, brittle fra...

متن کامل

Characterization of Viscoelastic Properties of Polymeric Materials through Nanoindentation

Nanoindentation is used to determine the dynamic viscoelastic properties of six polymer materials. It is shown that varying the harmonic frequency of the nanoindentation does not have any significant effect on the measured storage and loss moduli of the polymers. Agreement is found between these results and data from DMA testing of the same materials. Varying the harmonic amplitude of the nanoi...

متن کامل

Improvement of Strength Parameters of Sand Reinforced with Polymeric Fibers

Triaxial consolidated drained, unconfined compression, and CBR tests have been conducted in order to study the stress-strain, strength, and volume change characteristics of fine sand specimens reinforced by polymeric fibers made from carpet wastes. The variables are aspect ratio (length/width) and weight percentage of the fibers. The results indicate that the peak strength and total volume chan...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MRS Bulletin

سال: 2020

ISSN: 0883-7694,1938-1425

DOI: 10.1557/mrs.2020.257