Nanoindentation and Nanoscratching of Hard Coating Materials for Magnetic Disks
نویسندگان
چکیده
منابع مشابه
Permanent magnets and hard magnetic materials
This review deals with the definition and development of hard magnetic materials with special emphasis on more recent developments in this field. After discussing the fundamental properties of all hard magnetic materials, based on the intrinsic and extrinsic properties, some remarks on the history of hard magnetic materials and permanent magnets are given. The important hard ferrites are only b...
متن کاملNanoindentation studies of materials
have recognized that surface contacts between materials are highly dependent on their mechanical properties1,2. Many different indentation and impression tests have been developed in an effort to measure such mechanical properties from a contact of known geometry. In the past two decades, however, a veritable revolution has occurred in indentation testing, owing to the development of new sensor...
متن کاملAnalysis of onset of dislocation nucleation during nanoindentation and nanoscratching of InP
Nanoindentation and nanoscratching of an indium phosphide (InP) semiconductor surface was investigated via contact mechanics. Plastic deformation in InP is known to be caused by the nucleation, propagation, and multiplication of dislocations. Using selective electrochemical dissolution, which reveals dislocations at the semiconductor surface, the load needed to create the first dislocations in ...
متن کاملARTICLES Analysis of onset of dislocation nucleation during nanoindentation and nanoscratching of InP
Nanoindentation and nanoscratching of an indium phosphide (InP) semiconductor surface was investigated via contact mechanics. Plastic deformation in InP is known to be caused by the nucleation, propagation, and multiplication of dislocations. Using selective electrochemical dissolution, which reveals dislocations at the semiconductor surface, the load needed to create the first dislocations in ...
متن کاملRoughness Model for Adhesion Testing of Pharmaceutical Coating Materials
Objective Roughness is the main parameter in interlocking bonding mechanism. Yet there is no model designed to evaluate the effect of surface roughness on adhesion of coating materials in pharmaceutical sciences. Materials and Methods In this study polymethyl metacrylate spherical beads with different sizes were poured into 10 mm mold, then it was pressed by hand screw and finally heated to 141...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MRS Proceedings
سال: 1994
ISSN: 0272-9172,1946-4274
DOI: 10.1557/proc-356-767