Copper Tube Pitting in Santa Fe Municipal Water Caused by Microbial Induced Corrosion

Many copper water lines for municipal drinking water in Santa Fe, New Mexico USA, have developed pinhole leaks. The pitting matches the description of Type I pitting of copper, which has historically been attributed to water chemistry and to contaminants on the copper tubing surface. However, more recent studies attribute copper pitting to microbial induced corrosion (MIC). In order to test for...

متن کامل

Numerical Simulation of Material Strength Deterioration due to Pitting Corrosion

Pitting corrosion is an insidious form of localized corrosion a ecting characteristics of various engineering metallic alloys. Currently very limited literature exists with regard to systematic characterization of pitted surfaces or the efficient use of numerical methods to assess its effect, i.e. fatigue life reduction caused by the state of a corroded specimen and particularly through the stu...

متن کامل

Intergranular pitting corrosion of CoCrMo biomedical implant alloy.

CoCrMo samples of varying microstructure and carbon content were electrochemically corroded in vitro and examined by scanning electron microscopy and electron backscatter diffraction techniques. The rate of corrosion was minimized (80% reduction from icorr = 1396 nA/cm(2) to icorr = 276 nA/cm(2) ) in high-carbon CoCrMo alloys which displayed a coarser grain structure and partially dissolved sec...

متن کامل

Probabilistic Pitting Corrosion Risk Assessment of Welded Offshore Steel Pipelines

Steel structures continuously exposed to offshore marine environments are prone to corrosion. This can be of major economic and perhaps of environmental significance. The risk of these scenarios occurring can be assessed using good quality data, good quality corrosion and pitting models and structural reliability assessment. Recently, improved models for the prediction of longer term corrosion ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Zairyo-to-Kankyo

سال: 2008

ISSN: 0917-0480,1881-9664

DOI: 10.3323/jcorr.57.172