Morphology Evolution of γ′ Precipitates for Wrought Ni-Based Superalloys
نویسندگان
چکیده
منابع مشابه
Interdiffusion Behavior of Pt-Diffused γ+γ' Coatings on Ni-Based Superalloys
Platinum-diffused γ+γ' coatings (~20 at.% Al, ~22 at.% Pt) were synthesized on René 142 and René N5 Ni-based superalloys by electroplating the substrates with ~7 μm of Pt, followed by an annealing treatment in vacuum at 1175°C. In order to study the compositional and microstructural evolution of these coatings at elevated temperatures, interdiffusion experiments were carried out on coated speci...
متن کاملAutomated Identification and Characterization of Secondary & Tertiary Γ’ Precipitates in Nickel-based Superalloys (preprint)
The public reporting burden for this collection of information is estimated to average 1 hour per response, including the time for reviewing instructions, searching existing data sources, gathering and maintaining the data needed, and completing and reviewing the collection of information. Send comments regarding this burden estimate or any other aspect of this collection of information, includ...
متن کاملModeling displacive–diffusional coupled dislocation shearing of c0 precipitates in Ni-base superalloys
In Ni-base superalloys, superlattice extrinsic stacking fault (SESF) shearing of c0 precipitates involves coupled dislocation glide and atomic diffusion. A phase-field model is developed to study this process, in which the free energy of the system is formulated as a function of both displacement and long-range order parameter. The free energy surface is fitted to various fault energy data obta...
متن کاملMODELLING THE MATERIAL PROPERTIES AND BEHAVIOUR OF Ni-BASED SUPERALLOYS
At the last two Superalloy meetings at Seven Springs, work on the development of thermodynamic modelling tools for application to multi-component Ni-based superalloys has been presented. Such modelling has become quite widespread, providing significant benefit. However, its applicability often falls short from directly providing the information that is actually required and, by itself, cannot b...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MATERIALS TRANSACTIONS
سال: 2020
ISSN: 1345-9678,1347-5320
DOI: 10.2320/matertrans.mt-m2020183