Molybdenum recovery from steelmaking dust with an alkali water leaching process.
نویسندگان
چکیده
منابع مشابه
Recovery of metals from waste printed circuit boards by supercritical water pre-treatment combined with acid leaching process.
Waste printed circuit boards (PCBs) contain a large number of metals such as Cu, Sn, Pb, Cd, Cr, Zn, and Mn. In this work, an efficient and environmentally friendly process for metals recovery from waste PCBs by supercritical water (SCW) pre-treatment combined with acid leaching was developed. In the proposed process, waste PCBs were pre-treated by SCW, then the separated solid phase product wi...
متن کاملInvestigation on selective rhenium leaching from molybdenite roasting flue dusts
The possibility of selective leaching process was investigated during molybdenite flue dust leaching to recover its rhenium content. The results show that addition of alcohols to water makes the medium less favorable for molybdenum transfer into aqueous phase. On the other hand, addition of small amounts of alcohols (5-15%) makes a noticeable separation of rhenium over molybdenum, but by increa...
متن کاملSustainable Steelmaking by Process Integration
................................................................................................................... IV APPENDED PAPERS .................................................................................................... VI RELATED PUBLICATIONS........................................................................................ VII TABLE OF CONTENTS ..............................
متن کاملDecolorization of Molasses Waste Water from an Alcoholic Fermentation Process with Phanerochaete Chrysosporium Involvement of Ligninase
Waste water from a molasses alcoholic fermentation plant (MWW) was treated biologically with Phanerochaete chrysosporium. The ability of this white-rot fungus to degrade the dark colored pigments present in MWW and the consequent decrease the effluent's color was examined. The Optimum concentration of MWW for color removal was determined and set at the ratio of 1:10. The color changes durin...
متن کاملcopper and nickel recovery from electroplating sludge by the process of acid-leaching and electro-depositing
in this work, we developed a method which combined the processes of acid-leaching, ammonium jarosite precipitating and electro-depositing to recover copper and nickel from electroplating sludge. residual sludge from an electroplating plant located in qingdao was used for acid-leaching, and more than 95% of copper, nickel, zinc, chromium and iron were extracted from the sludge. after acid-leachi...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Shigen-to-Sozai
سال: 1990
ISSN: 0916-1740,1880-6244
DOI: 10.2473/shigentosozai.106.479