Microstructures and Charpy Fracture Surface Characteristics of Aged Refractaloy 26 Type Alloy and Inconel X Type Alloy

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Superplastic Forming of Inconel Alloy 718spf

Superplasticforming (SPF) has become an important manufacturing method for aerospace and fuselage components. The basic reasons for the popularity of this process are reviewed and the compatibilityoffine-grained INCONELB alloy71 8SPF@ to superplasticforming are presented in this paper. The temperature limitations of current aluminum and titanium alloys employed in SPF parts for gas turbine comp...

متن کامل

Characteristics of Biomedical Beta-Type Titanium Alloy Subjected to Coating

Beta-type titanium alloys used in biomedical applications have been developed all over the world. In particular, Ti-29Nb-13Ta-4.6Zr alloy (TNTZ) is one of beta-type titanium alloys for biomedical applications that has been developed by the authors in Japan. Although TNTZ is composed of non-toxic elements such as niobium, tantalum, and zirconium, it still lacks bioactivity, which is the ability ...

متن کامل

High temperature characteristics and solidification microstructures of dental metallic materials. Part II. ADAS Type 3 gold alloy.

Previously, high temperature properties of the silver-palladium-copper-gold alloy were investigated. In this study, the thermal expansion percentage and coefficient, and high temperature strengths of ADAS Type 3 gold alloy were investigated up to the liquidus temperature. Furthermore, microstructural and compositional changes in the solid/liquid dual phase were studied. The following conclusion...

متن کامل

TENSILE AND FRACTURE CHARACTERISTICS OF A SIC- PARTICLE-REINFORCED 7075 ALUMINIUM ALLOY

Fracture behavior of a 7075 aluminium alloy reinforced with 15 Vol%. SiC particles was studied after T6 and annealing heat treatments under uniaxial tensile loading at room temperature. The scanning electron microscopy of fractured surfaces and EDS analysis showed:, that fracture mechanism changed from due mainly to fractured particle in T6 condition to interface decohesion in samples in anneal...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Tetsu-to-Hagane

سال: 1970

ISSN: 0021-1575,1883-2954

DOI: 10.2355/tetsutohagane1955.56.14_1867