Microstructure control during twin roll casting of an AZ31 magnesium alloy
نویسندگان
چکیده
منابع مشابه
Effect of Rolling Route on Microstructure and Tensile Properties of Twin-Roll Casting AZ31 Mg Alloy Sheets
Twin-roll casting AZ31 Mg alloy sheets have been fabricated by normal unidirectional-rolling, head-to-tail rolling, and clock-rolling, respectively. It has been demonstrated that head-to-tail rolling is the most effective to refine the microstructure and weaken the basal texture among the three rolling routes. Excellent integrated tensile properties can be obtained by the head-to-tail rolling. ...
متن کاملTowards Superplastic Forming of Az31 Magnesium Alloy with Controlled Microstructure
A recent study on post-superplastic forming properties has shown that heating time prior to testing has a major effect on the post-forming properties of superplastically-formed AZ31 Magnesium alloy sheets. To this point, there has been very little examination into the effects of pre-heating or annealing on superplastic forming. In this work, these effects are examined using AZ31 Mg alloy sample...
متن کاملMicrostructure analysis of AZ31 magnesium alloy welds using phase-field models
We use phase-field models to characterize the microstructure present in magnesium AZ31 alloy solidified under welding conditions. We focus our attention on the study of the conditions under which a columnar-to-equiaxed transition (CET) is observed in resistance spot welds. Our simulations show how the size and shape of the columnar and equiaxed regions depend on factors such as cooling rate, te...
متن کاملInfluence of Accumulative Roll Bonding on the Texture and Tensile Properties of an AZ31 Magnesium Alloy Sheets
Deformation behaviour of rolled AZ31 sheets that were subjected to the accumulative roll bonding was investigated. Substantially refined microstructure of samples was achieved after the first and second pass through the rolling mill. Sheets texture was investigated using an X-ray diffractometer. Samples for tensile tests were cut either parallel or perpendicular to the rolling direction. Tensil...
متن کاملAnodizing of Magnesium Alloy Az31 by Alkaline Solution
-Anodizing of AZ 31 Mg alloy was investigate in 3M KOH solution for 10, 20 and 30min. at constant voltage of 5V. Atomic force microscope (AFM) used to investigate the roughness of anodic film formed on the surface while the scanning electron microscope (SEM) was used to determine the morphology of the anodic film, it was found that the roughness of the anodic film is mainly depend on the anodiz...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: IOP Conference Series: Materials Science and Engineering
سال: 2012
ISSN: 1757-899X