Microstructure and Stress Corrosion Cracking Behavior of the Weld Metal in Alloy 52-A508 Dissimilar Welds

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Evaluation of Corrosion Behavior of AISI 347 Stainless Steel to ASTM A335 Low Alloy Steel Dissimilar Welds

In the present study, the corrosion behavior of AISI 347 austenitic stainless steel to ASTM A335 low alloy steel dissimilar joint was investigated. For this purpose, two filler metals, ER309L and ERNiCr-3, were selected to be used during the gas tungsten arc welding process. To investigate the corrosion behavior of the joints after welding, the specimens were tested in 3.5% sodium chloride solu...

متن کامل

Stress Corrosion Cracking Susceptibility of 304L Substrate and 308L Weld Metal Exposed to a Salt Spray

304 stainless steels (SS) were considered as the materials for a dry storage canister. In this study, ER (Electrode Rod) 308L was utilized as the filler metal for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. The electron backscatter diffraction (EBSD) map was used to identify the inherent microstr...

متن کامل

Evaluation of the Melted Zone Microstructure in the Interface of the Dissimilar Weld between A335 Low Alloy Steel and ER309L Filler Metal by Gas Tungsten Arc Welding

In the present study, the microstructure and mechanical properties of the dissimilar welding between ASTM A335 low alloy steel and ER309L austenitic stainless steel were investigated using the gas tungsten arc welding process. The welding of dissimilar materials between ASTM A335 low alloy steel and ER309L austenitic stainless steel was found to have a significant effect on the microstructure w...

متن کامل

the evaluation of corrosion behavior of aisi 347 stainless steel to astm a335 low alloy steel dissimilar welds

in the present study, the corrosion behavior of aisi 347 austenitic stainless steel to astm a335 low alloysteel dissimilar joint was investigated. for this purpose, two filler metals, er309l and ernicr-3, were selected to be used during the gas tungsten arc welding process. to investigate the corrosion behavior of the joints after welding, the specimens were tested in 3.5% sodium chloride solut...

متن کامل

Effects of Microstructure and Bond Quality on the Ultrasonic Evaluation of Dissimilar Metal Friction Welds

During the last several years we have been investigating ultrasonic techniques for evaluating the quality of solid state weld interfaces [1 ,2]. Promising results have been obtained on a variety of different solid state welds by extracting features from the ultrasonic waveforms and applying pattern recognition algorithms to separate acceptable from unacceptable welds. In general, the primary di...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MATERIALS TRANSACTIONS

سال: 2011

ISSN: 1345-9678,1347-5320

DOI: 10.2320/matertrans.m2010294