Formation and Evaluation of Oxidation Behavior of Zirconia- Aluminide Coating on Nickel- Based Alloy

Practical applications of thermal barrier coatings with aluminide bond-coats are limited due to oxide scale spallation of the aluminide coating under applied thermal stresses. Considering the positive effects of oxygen-active elements or their oxides on the high temperature oxidation behavior, in this research zirconia was introduced into an aluminide coating. For this purpose, a Watts type bat...

متن کامل

Formation Mechanism of Silicon Modified Aluminide Coating on a Ni-Base Superalloy

Formation mechanism of silicon modified aluminide coating applied on a nickel base super alloy IN-738 LC by pack cementation process was the subject of investigation in this research. Study of the microstructure and compositions of the coating was carried out, using optical and scanning electron microscopes, EDS and X-ray diffraction (XRD) techniques. The results showed that due to low partial ...

متن کامل

Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483

In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

متن کامل

Cyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy

In this study, aluminide coating was employed to enhance the high-temperature cyclic oxidation of Rene-80 superalloy at 950ºC. The microstructural aspects and phase constituents of samples were  investigated with scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. The result of oxidation tests showed that the weight gain in the uncoated sample was considerably higher than...

متن کامل

Nickel Base Superalloy Rene®80 – The Effect of High Temperature Cyclic Oxidation on Platinum-Aluminide Coating Features

Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on beha...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Chinese Journal of Aeronautics

سال: 2012

ISSN: 1000-9361

DOI: 10.1016/s1000-9361(11)60451-2