Microstructure and Notch Properties of Heat-Treated Ti-4.5Al-3V-2Mo-2Fe Laser Welds

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Influence of heat treatment on the microstructure and properties of laser welds in 8090

An investigation into the weldability of the Al-Li-Cu-Mg-Zr alloy 8090 using a CO, laser indicates that the grain structure and microstructure of the weld zone are sensitive to the post-weld heat treatment. If a slow heating rate of 1Krnin-I to the solution treatment temperature is used the formation of P' (AIJr) dispersoids is promoted which leads to a uniformly small grain size within the fus...

متن کامل

Prediction of cooling rate and microstructure in laser spot welds

Theoretical and experimental investigations have been carried out to examine the in uence of laser power and on time on the weld thermal cycle and weld metal microstructure and hardness during laser spot welding of low alloy steel. A transient heat transfer model that takes into account the temperature dependence of material properties and latent heat of phase transformation is employed to sim...

متن کامل

control of the optical properties of nanoparticles by laser fields

در این پایان نامه، درهمتنیدگی بین یک سیستم نقطه کوانتومی دوگانه(مولکول نقطه کوانتومی) و میدان مورد مطالعه قرار گرفته است. از آنتروپی ون نیومن به عنوان ابزاری برای بررسی درهمتنیدگی بین اتم و میدان استفاده شده و تاثیر پارامترهای مختلف، نظیر تونل زنی(که توسط تغییر ولتاژ ایجاد می شود)، شدت میدان و نسبت دو گسیل خودبخودی بر رفتار درجه درهمتنیدگی سیستم بررسی شده اشت.با تغییر هر یک از این پارامترها، در...

15 صفحه اول

Effect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint

In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...

متن کامل

Effect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint

In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: MATERIALS TRANSACTIONS

سال: 2009

ISSN: 1345-9678,1347-5320