Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting

نویسندگان

چکیده

The aim of this study is to evaluate the wear and micro hardness a Ti-6Al-4V matrix reinforced with 10% 15% tungsten carbide particle (WCp) composite manufactured using squeeze casting process. Optical microscopy used determine microstructures composite. A pin-on-disc test equipment Vickers at atmospheric temperature were examine behaviour rate, CoF, qualities primed samples. Loads 10 N 80 N, velocities 4 m/s, distances 1000 m 2000 are considered for analyzing composites. rate values 25.683 WCp, 30.957 37.683 20% WCp. scanning electron microscope (SEM) utilized worn surface For CoF 0.82 0.87, WC, 0.88 0.956. 692 VHN WCp 835 microstructure, SEM images, coefficient friction, TMCs totaling reinforcing possessions discovered be improved.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications.

The microstructure and mechanical behavior of simple product geometries produced by layered manufacturing using the electron beam melting (EBM) process and the selective laser melting (SLM) process are compared with those characteristic of conventional wrought and cast products of Ti-6Al-4V. Microstructures are characterized utilizing optical metallography (OM), scanning electron microscopy (SE...

متن کامل

Microstructure and Mechanical Behavior of Porous Ti–6Al–4V Processed by Spherical Powder Sintering

Reducing the stiffness of titanium is an important issue to improve the behavior of this material when working together with bone, which can be achieved by generating a porous structure. The aim of this research was to analyze the porosity and mechanical behavior of Ti-6Al-4V porous samples developed by spherical powder sintering. Four different microsphere sizes were sintered at temperatures r...

متن کامل

Microstructure and Mechanical Properties of Direct Metal Laser Sintered Ti- 6al-4v

Direct metal laser sintering (DMLS) is a selective laser melting (SLM) manufacturing process that can produce near net shape parts from metallic powders. A range of materials are suitable for SLM; they include various metals such as titanium, steel, aluminium, and cobalt-chrome alloys. This paper forms part of a research drive that aims to evaluate the material performance of the SLM-manufactur...

متن کامل

Ti-6Al-4V Synthesized by Mechanical Alloy Method and Mechanical and Bioactivity Properties of Ti-6Al-4V/HA-Clay Nano composite

Nowadays, titanium-based alloys are among the most attractive metallic materials for biomedical applications (as implants) due to their non-biodegradability, low density, good mechanical properties as well as their good biocompatibility. Hydroxyapatite (Ca10 (PO4)6(OH)2, HA) has been widely used for biomedical applications due to its bioactive, biocompatible and osteoconductive properties. Firs...

متن کامل

Fatigue of Ti-6Al-4V

Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Nanomaterials

سال: 2022

ISSN: ['1687-4110', '1687-4129']

DOI: https://doi.org/10.1155/2022/6381265