Microstructure and creep strength of different γ/γ′-strengthened Co-base superalloy variants
نویسندگان
چکیده
منابع مشابه
Creep Crack Growth Simulation of Ni-base Superalloy
The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...
متن کاملDependence of Creep Performance and Microstructure Evolution on Solution Cooling Rate in a Polycrystalline Superalloy
It is well known that the solution cooling rate has a great effect on the creep life of superalloys. In this research, three typical cooling rates were applied to generate different distributions of γ’ precipitates for creep tests. Ingots used to make specimens were manufactured by hot extrusion, and the master alloy had the composition of an FGH4096 power metallurgy superalloy. SEM and SESD we...
متن کاملInvestigation of the Effect of Homogenization Treatment on Distribution of Alloying Elements, Microstructure and Hardness of Co-Al-W-Ti-Ta-Base Superalloy
The aim of this study was to investigate the effect of temperature and time of homogenization treatment on the microstructure, distribution of alloying elements and hardness of the novel Co-based superalloy Co-7Al-7W-4Ti-2Ta. For this purpose, the specimens were first homogenized at 1250 and 1300 °C for 2, 4, 6 and 8 hours and then water-cooled. Subsequently, the specimens were subjected to har...
متن کاملModeling the Temperature-dependence of Tertiary Creep Damage of a Directionally Solidified Ni-base Superalloy
Directionally solidified (DS) Ni-base superalloys have become a commonly used material in gas turbine components. Controlled solidification during the material manufacturing process leads to a special alignment of the grain boundaries within the material. This alignment results in different material properties dependent on the orientation of the material. When used in gas turbine applications t...
متن کاملA Coupled Creep-plasticity Model for Residual Stress Relaxation of a Shot-peened Nickel-base Superalloy
A COUPLED CREEP-PLASTICITY MODEL FOR RESIDUAL STRESS RELAXATION OF A SHOT-PEENED NICKEL-BASE SUPERALLOY Name: Dennis Justin Buchanan University of Dayton, 2007 Advisor: Dr. R. A. Brockman Shot peening has been employed in numerous industries for decades to impart beneficial compressive residual stresses on the surface of metal components. Compressive residual stresses retard initiation of surfa...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Scripta Materialia
سال: 2010
ISSN: 1359-6462
DOI: 10.1016/j.scriptamat.2010.08.036