Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483
In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...
متن کاملEffect of Thermal History on Microstructural Changes in Aluminized Nickel-Based Single-Crystal Superalloy
The effect of the thermal history on microstructural changes in aluminized and Pt-aluminized Ni-based single-crystal superalloys was investigated. The superalloy substrates were first electropolished to get rid of the residual surface strain. Then, Pt was electrodeposited and vacuum annealing was conducted for some of the substrates, and aluminized and Pt-aluminized specimens were prepared usin...
متن کاملIn- and Out-of Phase Thermomechanical Fatigue of a Ni-Based Single-Crystal Superalloy
In this study, the difference between in-phase (IP) and out-of-phase (OP) thermomechanical fatigue (TMF) cycling from 100 to 750 ◦C has been investigated for the Ni-based single-crystal superalloy MD2. In addition, two different crystal orientations were studied, the 〈001〉 and 〈011〉 orientations respectively. When comparing IP and OP TMF lives, a strain range dependency is found for the 〈001〉 d...
متن کاملSimulation of oxidation-nitridation-induced microstructural degradation in a cracked Ni- based superalloy at high temperature
In turbine engines, high temperature components made of superalloys may crack in a creep process during service. With the inward flux of the gases, e.g. oxygen and nitrogen, along those cracks, the microstructure of the superalloy substrate nearby the cracks may degrade by internal oxidation and nitridation. The aim of this study is to investigate and simulate the oxidation-nitridation-induced ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MATERIALS TRANSACTIONS
سال: 2006
ISSN: 1345-9678,1347-5320
DOI: 10.2320/matertrans.47.1665