Microstructural Features and Mechanical Properties after Industrial Scale ECAP of an Al 6060 Alloy
نویسندگان
چکیده
منابع مشابه
Investigation of the Physical and Mechanical Properties of Silicon Carbide Prepared on an Industrial Scale
In this study, an industrial polycrystalline SiC tile was successfully sintered by pressureless sintering at 2150°C for 1 hour. The physical and mechanical properties of silicon carbide including density, hardness, bending strength, and fracture toughness were evaluated. The results indicated that the mentioned properties were 3.08 g.cm-3, 2503 HV0, 249.3 MPa, and 1.23 MPam0.5</...
متن کاملdetermination of some physical and mechanical properties red bean
چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...
15 صفحه اولMicrostructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evolutions during annealing
Microstructures and mechanical properties of equal-channel angular pressing (ECAP) processed and naturally aged ultrafine grained (UFG) and coarse grained (CG) 7075 Al alloys as well as their evolutions during annealing were investigated. After the same natural aging, the tensile yield strength, ultimate strength, and microhardness of the UFG samples were 103%, 35%, and 48% higher, respectively...
متن کاملEffect of Mechanical Alloying and Sintering on Phase Transformation, Microstructural Evolution, Mechanical Properties and Density of Zr-Cr Alloy
The purpose of present research was production ofZr-based alloy as the nuclear fuel cladding by mechanical alloying (MA) and sintering process. Firstly, Zr and Cr powders were mechanically alloyed to produce the refractory and hard Zr-10 wt% Cr alloy, and then, the powder mixtures were consolidated by press and following sintering at temperature of 800˚C min. The phase evolution, microstructura...
متن کاملINVESTIGATION OF MICROSTRUCTURAL AND MECHANICAL PROPERTIES OF 7075 AL ALLOYPREPARED BY SIMA METHOD
The microstructure and mechanical properties of 7075 wrought aluminum alloy produced by strain induced melt activation (SIMA) route were investigated.Also liquid volume fraction measurement was studied by three procedures. Remelting process was carried out in the range of 560 to 610 °C for 20 min holding. The microstructure in the semi-solid state consists of fine spherical solid grains surroun...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science Forum
سال: 2010
ISSN: 1662-9752
DOI: 10.4028/www.scientific.net/msf.667-669.1153