Microstructural Characterization and Phase Separation Sequences During Solidification of Ni3Al-Based Superalloy
نویسندگان
چکیده
منابع مشابه
Synthesis and Characterization of Nanocrystalline Ni3Al Intermetallic during Mechanical Alloying Process
In this research, formation of nanocrystalline Ni3Al intermetallic from Ni and Al elemental powders by mechanical alloying (MA) process and its characterization was investigated. Therefore, the evolutions in microstructure such as phase transformation, oxidation in air and introduction of Fe impurity from milling media after MA were evaluated using XRD, Rietveld refinement, TEM, SEM, EDS and IC...
متن کاملPhase-field Modeling with CALPHAD and CVM for Microstructural Evolution of Ni-base Superalloy
To perform a quantitative simulation using the Phase Field Method (PFM) in a real alloy system, a new strategy of modeling the microstructure evolution of Ni-base superalloy is proposed in the present paper. In this strategy, the Calculation Phase Diagram (CALPHAD) method and Cluster Variation Method (CVM) are combined with the PFM, in which the four sub-lattice model is used to evaluate the fr...
متن کاملSolidification Behavior of Polymer Solution during Membrane Preparation by Thermally Induced Phase Separation
The solidification behavior of poly(vinylidene fluoride) (PVDF) solution during membrane preparation by thermally induced phase separation (TIPS) was investigated. Apparatus newly developed in our laboratory was used to quantitatively measure membrane stiffness during phase separation. In this apparatus, a cooling polymer solution, placed on a stage, is moved upwards and the surface of the poly...
متن کاملDirectional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field
A Ni-based superalloy CMSX-6 was directionally solidified at various drawing speeds (5–20 μm·s−1) and diameters (4 mm, 12 mm) under a 0.5 T weak transverse magnetic field. The results show that the application of a weak transverse magnetic field significantly modified the solidification microstructure. It was found that if the drawing speed was lower than 10 μm·s−1, the magnetic field caused ex...
متن کاملsynthesis and characterization of some macrocyclic schiff bases
ماکروسیکلهای شیف باز از اهمیت زیادی در شیمی آلی و دارویی برخوردار می باشند. این ماکروسیکلها با دارابودن گروه های مناسب در مکانهای مناسب می توانند فلزاتی مثل مس، نیکل و ... را در حفره های خود به دام انداخته، کمپلکسهای پایدار تولید نمایند. در این پایان نامه ابتدا یک دی آلدئید آروماتیک از گلیسیرین تهیه می شود و در مرحله بعدی واکنش با دی آمینهای آروماتیک و یا آلیفاتیک در رقتهای بسیار زیاد منجر به ت...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Acta Metallurgica Sinica (English Letters)
سال: 2017
ISSN: 1006-7191,2194-1289
DOI: 10.1007/s40195-017-0634-z