Microstructural and Electrical Properties of Sn-Modified BaTiO3 Lead-Free Ceramics by Two-Step Sintering Method

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrical properties of lead-free 0.98(Na0.5K0.5)NbO3-0.02Ba(Zr0.52Ti0.48)O3 piezoelectric ceramics by optimizing sintering temperature

Lead-free 0.98(Na0.5K0.5)NbO3-0.02Ba(Zr0.52Ti0.48)O3 [0.98NKN-0.02BZT] ceramics were fabricated by the conventional mixed oxide method with sintering temperature at 1,080°C to 1,120°C. The results indicate that the sintering temperature obviously influences the structural and electrical properties of the sample. For the 0.98NKN-0.02BZT ceramics sintered at 1,080°C to 1,120°C, the bulk density i...

متن کامل

Sintering of Lead-Free Piezoelectric Sodium Potassium Niobate Ceramics

The potassium sodium niobate, K0.5Na0.5NbO₃, solid solution (KNN) is considered as one of the most promising, environment-friendly, lead-free candidates to replace highly efficient, lead-based piezoelectrics. Since the first reports of KNN, it has been recognized that obtaining phase-pure materials with a high density and a uniform, fine-grained microstructure is a major challenge. For this rea...

متن کامل

Structural and Electrical Properties of BNT-BT0.08 Ceramics Processed by Spark Plasma Sintering

(Bi0.5Na0.5)TiO3 doped with 8 mol % BaTiO3 powder (BNT-BT0.08), prepared by sol-gel method was compacted and sintered by Spark Plasma Sintering (SPS) process. The influence of SPS temperature on the densification of BNT-BT0.08 ceramic was investigated. Starting from sol-gel nanopowder of BNT-BT containing 8 mol % BaTiO3 with an average particles size of about 30 nm, were obtained ceramics with ...

متن کامل

Processing, Mechanical and Optical Properties of Additive-Free ZrC Ceramics Prepared by Spark Plasma Sintering

In the present study, nearly fully dense monolithic ZrC samples are produced and broadly characterized from microstructural, mechanical and optical points of view. Specifically, 98% dense products are obtained by Spark Plasma Sintering (SPS) after 20 min dwell time at 1850 °C starting from powders preliminarily prepared by Self-propagating High-temperature Synthesis (SHS) followed by 20 min bal...

متن کامل

Enhanced dielectric and piezoelectric properties of xBaZrO3-(12x)BaTiO3 ceramics

xBaZrO3-(1!x)BaTiO3 solid solutions (x 1⁄4 0, 0.04, 0.06, 0.08, 0.12, and 0.18) synthesized via conventional solid state reaction method exhibit piezoelectric coefficients comparable to those of “hard” PZT-8, PZT-4, and even “soft” PZT-5A. Doping also improves the poling efficiency of xBaZrO3-(1!x)BaTiO3 ceramics. Study of temperature dependence of the dielectric and piezoelectric properties re...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Advances in Materials Science and Engineering

سال: 2018

ISSN: 1687-8434,1687-8442

DOI: 10.1155/2018/9048062