Mechanical response of aluminum 7075 with heat treatment and exfoliation corrosion

نویسندگان

چکیده

The present investigation was focussed to evaluate the mechanical properties of AA7075 subjected corrosion and heat treatment. Exfoliation has been used infuse rapid on material coupled with high temperature subsequent low-temperature aging (HLA). It found that localized pit formation occurs HLA exposure durations substantial inter-granular changes cracks. Significant reduction in observed HLA-treated samples corrosion. material’s stiffness increased due HLA, again within corrosive environment, a decreasing trend immersion durations. A series simple one-dimensional linear polynomial equations were developed determine

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Aging and Mechanical Behavior of Be-Treated 7075 Aluminum Alloys

The present study was undertaken to investigate the effect of pre-aging and aging parameters (time and temperature) on the mechanical properties of Al-Mg-Zn (7075) alloys. Ultimate tensile strength, 0.5% offset yield strength and % elongation measurements were carried out on specimens prepared from cast and heat treated 7075 alloys. Aging treatments were carried out for the as solution treated ...

متن کامل

Aging and Mechanical Behavior of Be-Treated 7075 Aluminum Alloys

The present study was undertaken to investigate the effect of pre-aging and aging parameters (time and temperature) on the mechanical properties of Al-Mg-Zn (7075) alloys. Ultimate tensile strength, 0.5% offset yield strength and % elongation measurements were carried out on specimens prepared from cast and heat treated 7075 alloys. Aging treatments were carried out for the as solution treated ...

متن کامل

Effect of heat treatment on the grain structure and mechanical properties of Al-7075 friction stir weld

The fine grain structure of friction-stir welded aluminum alloys is unstable during post weld heat treatment and some grains abnormally grown. In this study, the sequence of abnormal grain growth during T6 heat treatment of Al-7075 friction-stir weld and its effect on mechanical properties of the weld was studied. The results showed that heat treatment in 510 ˚C resulted in drastic grain growth...

متن کامل

EFFECT OF T6 HEAT TREATMENT ON MECHANICAL PROPERTIES OF CERAMIC REINFORCED CASTED ALUMINUM ALLOY

Aluminium base alloy (Al-Cu-Si) was reinforced with silicon carbide (SiC) particles, in various percentage compositions from 0-20 wt%. Silicon carbide particle size of 20µm was selected. The molten slurry of SiC reinforced base aluminium metal was casted through green and dry sand casting methods and solidification process was carried out under ambient conditions. A selected population...

متن کامل

Effect of heat treatment on the grain structure and mechanical properties of Al-7075 friction stir weld

The fine grain structure of friction-stir welded aluminum alloys is unstable during post weld heat treatment and some grains abnormally grown. In this study, the sequence of abnormal grain growth during T6 heat treatment of Al-7075 friction-stir weld and its effect on mechanical properties of the weld was studied. The results showed that heat treatment in 510 ˚C resulted in drastic grain growth...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Today: Proceedings

سال: 2021

ISSN: ['2214-7853']

DOI: https://doi.org/10.1016/j.matpr.2021.05.081