In this work, a transparent nanostructured ceramic magnesium aluminate spinel (MgAl2O4) was fabricated by Spark Plasma Sintering (SPS) from commercial nano-powders at different temperatures (1300, 1350 and 1400 °C). The sintered samples were thoroughly examined to assess their microstructural, optical, mechanical properties. Various techniques such as SEM, AFM, spectrophotometer with an integrating sphere, instrumented Vickers indenter, Pin-on-Disk tribometer, scratch tester, sandblasting device employed characterize the samples. results indicated significant impact of sintering temperature on properties Particularly, T = °C exhibited highest Real In-line Transmission (RIT 72% 550 nm 80% 1000 nm). These demonstrated hardness value (HV 16.7 GPa) compared those 1300 15.6 15.1 GPa). measured fracture toughness increased substantially increasing temperature. Similarly, tribological study revealed that friction coefficient temperature, lowest wear rate. Additionally, tests confirmed influence spinels. Overall, presented best compromise in terms all evaluated

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

In-situ Fabrication of Transparent Magnesium Aluminate Spinel by Spark Plasma Sintering

Transparent polycrystalline spinel ceramic was fabricated without any sintering aids by spark plasma sintering method of a mixture of Al2O3 and MgO powders for only 10min soak at 1250°C. Densification, microstructure and optical transparency of spinel were examined. The spinel exhibits an in-line transmission of 55% for a visible-wavelength of 470nm and high hardness value of 2040 HV.

متن کامل

Effect of SiC nanoparticles addition on mechanical properties and wear resistance of cemented carbides fabricated by spark plasma sintering

WC-10Co cemented carbides containing 1 to 4 wt% SiC nanoparticles were prepared by spark plasma sintering. The effects of SiC content on microstructure, mechanical properties and wear resistance of the sintered materials were studied. Microstructural studies showed that SiC addition resulted in WC grain coarsening. In addition, the hardness decreased with increasing SiC content. However, the fr...

متن کامل

ZrB2-CNTs Nanocomposites Fabricated by Spark Plasma Sintering

ZrB₂-based nanocomposites with and without carbon nanotubes (CNTs) as reinforcement were prepared at 1600 °C by spark plasma sintering. The effects of CNTs on the microstructure and mechanical properties of nano-ZrB₂ matrix composites were studied. The results indicated that adding CNTs can inhibit the abnormal grain growth of ZrB₂ grains and improve the fracture toughness of the composites. Th...

متن کامل

Fabrication of Nanostructured Cu matrix Nanocomposites by High Energy Mechanical Milling and Spark Plasma Sintering

Spark plasma sintering (SPS) is a sintering process that is capable of sintering hard worked powders in short times. This technique was used to fabricate bulk Cu and Cu-SiC nanocomposites. Pure Cu and mixed powders of Cu including 4 vol% of SiC nanoparticles were mechanically alloyed for 25 h and sintered at 750˚C under vacuum condition by SPS method. Microstructures of the materials were chara...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Ceramics

سال: 2023

ISSN: ['2571-6131']

DOI: https://doi.org/10.3390/ceramics6020072