Mechanical and tribological properties of WO2.9 and ZrO2 + WO2.9 composites studied by nanoindentation and reciprocating wear tests

نویسندگان

چکیده

Oxygen vacancies in WO2.9 yield to formation of easy shear planes and they can potentially be applied boundary lubrication conditions for reducing friction. Mechanical tribological properties pulsed electric current sintered monolithic were studied by nanoindentation nanoscratch, the composites ZrO2 + with reciprocating wear tests. Hardness at 25 °C was ~11 GPa reduced elastic modulus ~150 GPa. The ploughing dominated coefficient friction as between 0.09 0.24 when measured against a Berkovich diamond tip. composite n-ZrO2 10 vol% presented lowest CoF, rate 10?10 mm3/Nm under N load alumina ball (6 mm diameter) due acting solid lubricant.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

Mechanical and Wear Properties of Al-Nip Composites Produced by ARB Process

In this research, Al-Ni particle composite strips are formed by accumulative roll bonding (ARB) process using Al strips and Ni powder. The rule of ARB cycles and volume percentage (Vol%) of Ni powder on the microstructure, wear resistance and mechanical properties of the formed composites are investigated. According to the tensile test results, the yield stress and tensile strengths of the Al -...

متن کامل

some properties of fuzzy hilbert spaces and norm of operators

in this thesis, at first we investigate the bounded inverse theorem on fuzzy normed linear spaces and study the set of all compact operators on these spaces. then we introduce the notions of fuzzy boundedness and investigate a new norm operators and the relationship between continuity and boundedness. and, we show that the space of all fuzzy bounded operators is complete. finally, we define...

15 صفحه اول

Tribological Behavior and Mechanical Properties of Graphene/PEEK Composites

PEEK has been implemented in various orthopaedic applications due to its many beneficial mechanical, tribological, and radiolucent properties. These properties can be further tailored by introducing fillers into the PEEK matrix. In this work, graphene has been incorporated due to its high mechanical resistance, intrinsic stiffness, and lubricating properties [2].

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Wear

سال: 2021

ISSN: ['0043-1648', '1873-2577']

DOI: https://doi.org/10.1016/j.wear.2021.203920