Mechanical and Thermal Fatigue Property of Sn Base Solder Alloys.
نویسندگان
چکیده
منابع مشابه
THERMAL FATIGUE RESISTANCES OF 356 AND 413 CAST Al ALLOYS
Abstract: Thermal fatigue is a stochastic process often showing considerable scatter even in controlled environments. Due to complexity of thermal fatigue, there is no a complete analytical solution for predicting the effect of this property on the life of various components, subjected to severe thermal fluctuations. Among these components, one can mention car cylinder, cylinder head and pi...
متن کاملMeasuring intrinsic elastic modulus of Pb/Sn solder alloys
Young’s modulus (E) values published in the literature for the eutectic Pb37/Sn63 and near eutectic Pb40/Sn60 solder alloy vary significantly. One reason for this discrepancy is different testing methods for highly rate sensitive heterogeneous materials, like Pb/Sn alloys, yield different results. In this paper, we study different procedures used to obtain the elastic modulus; analytically, by ...
متن کاملDevelopment of Sn-Zn-Al Lead-Free Solder Alloys
Fujitsu has implemented a company-wide effort to progressively reduce the use of lead (Pb) and eventually eliminate this environmental pollutant from its products. As part of this effort, we have developed a new lead-free solder that consists of tin (Sn), zinc (Zn), and aluminum (Al) and yet offers superior productivity and joint reliability. The new lead-free solder has a melting point equival...
متن کاملLow-Cycle Fatigue Characteristics of Sn-Based Solder Joints
Low-cycle, lap-shear fatigue behavior of Sn-based, Pb-free solder alloys, Sn3.5Ag, Sn-3.5Ag-Cu, Sn-3.5Ag-Bi, and Sn-0.7Cu, were studied at room temperature using specimens with printed circuit board (PCB)/solder/PCB structure under total displacement of ±10 μm, 12 μm, 15 μm, and 20 μm. The fatigue lives of various solder joint materials, defined as 50% load drop, were correlated with the fractu...
متن کاملInterfacial Reaction and Mechanical Properties of Sn-Bi Solder joints
Sn-Bi solder with different Bi content can realize a low-to-medium-to-high soldering process. To obtain the effect of Bi content in Sn-Bi solder on the microstructure of solder, interfacial behaviors in solder joints with Cu and the joints strength, five Sn-Bi solders including Sn-5Bi and Sn-15Bi solid solution, Sn-30Bi and Sn-45Bi hypoeutectic and Sn-58Bi eutectic were selected in this work. T...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Japan Institute of Electronics Packaging
سال: 2000
ISSN: 1343-9677,1884-121X
DOI: 10.5104/jiep.3.592