Wear behaviour of AA6061 aluminium alloy and its composites
This study investigates the wear resistance of four AA6061 MMCs together with the monolithic AA6061 alloy, all in the T6 condition, using a pin-on-disc test. In addition to the widely studied 20 vol.% Saffil MMCs, the present investigation considered a hybrid of 11% Saffil + 20% Sic, and a high volume fraction Sic, MMC. AA6061 + 60% Sic,. The wear behaviour against P400 Sic grit adhesive bonded...
متن کاملFretting wear in self-piercing riveted aluminium alloy sheet
Fretting wear in aluminium alloy AA5754 joined by self-pierce riveting (SPR), a relatively new fastening technique increasingly used in vehicle structures, has been investigated in this paper. Surface damages have been induced when a joint experienced a sinusoidal cyclic tension-tension load. Various degradation zones have been characterised in the contact surfaces between the aluminium sheets,...
متن کاملQUALITY CONTROL OF PRECIPITATION HARDENED ALUMINIUM ALLOY PARTS VIA EDDY-CURRENT NONDESTRUCTIVE EVALUATION
Precipitation hardening is the most common method in the strengthening of aluminium alloys. This method relies on the decrease of solid solubility with temperature reduction to produce fine precipitations which impede the movement of dislocations. The quality control of aluminium alloy specimens is an important concern of engineers. Among different methods, non-destructive techniques are the...
متن کاملTEM characterisation of near surface deformation resulting from lubricated sliding wear of aluminium alloy and composites
Aluminium alloy composites have been extensively investigated for use in tribo-contact applications, however little detailed literature exists on the sub-surface microstructural evolution as a result of lubricated sliding wear. In this study two un-reinforced alloys (2124 & 5056) and identical alloy composites, reinforced with 15vol.% MoSi2 intermetallic particles were produced by a powder meta...
متن کاملEffects of Solidification Time on Mechanical Properties and Wear Behaviour of Sand Cast Aluminium Alloy
An investigation was carried out to understand the effects of solidification time of the cylindrical specimen on hardness, wear rate and the coefficient of friction of Aluminium alloy (LM4). The commercially available LM4 Aluminium alloy was melted in a crucible furnace under argon atmosphere. The molten metal was poured into sand moulds having dissimilar size holes. The cast rods were tested f...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MM Science Journal
سال: 2015
ISSN: 1803-1269,1805-0476
DOI: 10.17973/mmsj.2015_12_201552