Mathematical Modeling of Heating and Strain Aging of Steel during High-Speed Wire Drawing

نویسندگان

چکیده

In this article, a mathematical model of the wire’s average temperature change in process multiple drawing on high-speed straight-line machines has been developed. The calculation results showed that wire during at speed up to 45 m/s could reach 400 °C. Deformation heating does not exceed 60 °C, and due sliding friction can 300 depending coefficient, which ranges from 0.05 0.15. strain rates under conditions modern 7000 s?1. Over course research, it was found there are no for occurrence dynamic deformation aging impurity atoms carbon, nitrogen oxygen. At same time, parameters drawing, created onset steel presence hydrogen atoms. Therefore, heat treatment pickling, is necessary exclude hydrogenation steel. It established order static prevent above 180–200

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Static Strain Aging Behavior of Low Carbon Steel Drawn Wire

The static strain aging is a phenomenon that can change the mechanical properties of low carbon steels. Thus, the static strain aging behavior of low carbon steel wires after drawing process is studied. To do so, the wires are austenitized at different temperatures and cooled in different rates. Then the wires are drawn and aged at a specific temperature and time. Before and after aging of each...

متن کامل

static strain aging behavior of low carbon steel drawn wire

the static strain aging is a phenomenon that can change the mechanical properties of low carbon steels. thus, the static strain aging behavior of low carbon steel wires after drawing process is studied. to do so, the wires are austenitized at different temperatures and cooled in different rates. then the wires are drawn and aged at a specific temperature and time. before and after aging of each...

متن کامل

Developing Very Fine Nanopearlitic Structure in a High Carbon Steel Wire before Drawing

The effects of steel wire patenting process parameters on very fine interlamellar spacing in the pearlitic steel wire were investigated and the optimized condition of the process was achieved. In this work, the initial nanopearlitic structure was obtained in a 0.72 wt% carbon steel wire before the wire drawing process. The results were the minimum interlamellar spacing of 35 nm and maximum ulti...

متن کامل

Effect of Strain Induced Martensite on the Deep Drawing Behavior of 304L Steel: Simulation and Experiment

Abstract In the present research, the behavior of 304L austenitic stainless steel in the deep drawing process has been studied at the room temperature through experimental and finite element simulation method. Magnetic method calibrated by XRD was used to measure induced-martensite. Martensite volume fraction in the various portion of the deep drawn cup under optimum Blank Holder Force (BHF) a...

متن کامل

consequence analysis of the leakage, ignition and explosion during high pressure sour gas injection process to the oil reservoir

there is no doubt that human being needs to become integrated with industry and industry needs to be progressed, daily. on the other hand, serious events in industrial units specially in oil industries has been shown that such damages and events are industry related ones. the consequence of such events and damages which resulted in chemical and poisoned explosions and loss of life and property ...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2022

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met12091472