Machining behavior of additively manufactured and cast-wrought nickel-based superalloy (IN 625)

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Additively Manufactured Porous Biomaterials and Implants

Recent advances in additive manufacturing (AM) techniques (otherwise known as 3D printing) have enabled fabrication of a new class of porous biomaterials (Figure 1) with arbitrarily complex and precisely controlled topologies that e.g. resemble the geometry and micro-architecture of (trabecular) bone. Since the geometry of scaffolds and biomaterials is an important factor in bone tissue regener...

متن کامل

Constitutive Model Based on Dynamic Recrystallization Behavior during Thermal Deformation of a Nickel-Based Superalloy

Peng Zhang 1, Cen Yi 1, Gang Chen 1, Heyong Qin 2 and Chuanjie Wang 1,* 1 School of Materials Science and Engineering, Harbin Institute of Technology at Weihai, Weihai 264209, China; [email protected] (P.Z.); [email protected] (C.Y.); [email protected] (G.C.) 2 Central Iron & Steel Research Institute, Beijing 100081, China; [email protected] * Correspondence: [email protected]; Tel.: +86-631-568...

متن کامل

Mechanical Properties of Additively Manufactured Thick Honeycombs

Honeycombs resemble the structure of a number of natural and biological materials such as cancellous bone, wood, and cork. Thick honeycomb could be also used for energy absorption applications. Moreover, studying the mechanical behavior of honeycombs under in-plane loading could help understanding the mechanical behavior of more complex 3D tessellated structures such as porous biomaterials. In ...

متن کامل

Cyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy

In this study, aluminide coating was employed to enhance the high-temperature cyclic oxidation of Rene-80 superalloy at 950ºC. The microstructural aspects and phase constituents of samples were  investigated with scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. The result of oxidation tests showed that the weight gain in the uncoated sample was considerably higher than...

متن کامل

Additively manufactured medical products – the FDA perspective

Additive manufacturing/3D printing of medical devices is becoming more commonplace, a 3D printed drug is now commercially available, and bioprinting is poised to transition from laboratory to market. Despite the variety of technologies enabling these products, the US Food and Drug Administration (FDA) is charged with protecting and promoting the public health by ensuring these products are safe...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Manufacturing

سال: 2018

ISSN: 2351-9789

DOI: 10.1016/j.promfg.2018.07.070