Machinability of Inconel 825 superalloy under dry cutting environment with application of uncoated WC-Co tool

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718

In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...

متن کامل

Investigation of Cutting Forces Superalloy Inconel 718

Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...

متن کامل

EDM machinability and dry sliding friction of WC-Co cemented carbides

A number of WC-Co cemented carbides with 6–12 wt. % Co were machined and surface finished by grinding or Electrical Discharge Machining (EDM). EDM was executed in deionised water through several consecutive gradually finer steps. Correlations between Material Removal Rate (MRR), surface finish and EDM parameters were derived. The quality and integrity of surface finishes were analysed by Scanni...

متن کامل

Machinability Investigation of Inconel 657 in High-speed Turning

A high strength nickel chromium alloy (50Cr-50Ni-Nb alloy), commonly referred to as IN-657, is specifically used for components in furnaces which are fired by low grade fuel oils containing high levels of vanadium, sodium and sulphur. The purpose of this study is to experimentally investigatethe effect of machining parameters on machinability in turning of Inconel 657. The considered parameters...

متن کامل

Assessment of Machinability of Metal Cutting

The assessments of machinability of metal cutting are called "indices" and are derived by comparative research. These indices are the relations of two identical parameters, such as is the allowable cutting speed. The assessments were obtained at a constant tool life of 60 min, at the appropriate tool life minimum costs and the efficient reporting of specific restrictions for finishing and rough...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Today: Proceedings

سال: 2021

ISSN: 2214-7853

DOI: 10.1016/j.matpr.2020.05.150