Low intrinsic thermal conductivity of Spark Plasma Sintered dense KNbO3 and NaNbO3 perovskite ceramics

نویسندگان

چکیده

The origin of low thermal conductivity in niobium-containing perovskites was investigated. Therefore, dense NaNbO3 and KNbO3 ceramics were sintered by spark plasma sintering. grain size the 1–10 μm range. ceramic has shown a stable circa 2.6 W m−1 K−1 from 373 to 1000 K KNbO3, values 2.5 plateau at 1.2 since 673 K. This value is lowest reported for an oxide presenting perovskite structure. such conductivities indicated be related with cation deficiency on A-site perovskites.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructure of spark plasma sintered TiB2 and TiB2–AlN ceramics

In this research study, the effects of aluminum nitride (AlN) additive on the densification behavior and microstructure development of titanium diboride (TiB2) based ceramic matrix composite were investigated. In this way, a monolithic TiB2 ceramic and a TiB2–5 wt% AlN ultrahigh temperature ceramic composite were fabricated by spark plasma sintering (SPS) proces...

متن کامل

Phase assembly and electrical conductivity of spark plasma 4 sintered CeO 2 – ZrO 2 ceramics 5

10 Abstract CexZr1-xO2 (x = 0.10, 0.16 and 0.33) nano11 crystalline powders were obtained by a two-step synthesis 12 technique and sintered by spark plasma sintering (SPS). As 13 consequence of the reduction of Ce to Ce species by 14 carbon in the graphite environment in SPS, phase assem15 blies including tetragonal, monoclinic and pyrochlore 16 phases were generated in the ceramics during the ...

متن کامل

Microstructure and Properties of Spark Plasma Sintered MoAlB Ceramics

Advisor: Bai Cui Molybdenum aluminum boride (MoAlB) is a ternary transition metal boride which has promising aeronautic and nuclear applications. It inheres excellent properties of the binary transitional metal borides (e.g., MoB, ZrB2) such as high melting temperature, high hardness, and thermal conductivity. Besides, MoAlB is superior to MoB because: (1) the Al element provides an oxidation r...

متن کامل

Microstructure of Spark Plasma-Sintered Silicon Nitride Ceramics

The microstructure and phase composition of the high-content Al2O3-Y2O3-doped spark plasma-sintered silicon nitride were investigated. Fully dense silicon nitride ceramics with a typical α-Si3N4 equiaxed structure with average grain size from 200 to 530 nm, high elastic modulus of 288 GPa, and high hardness of 2038 HV were spark plasma sintered (SPSed) at 1550 °C. Silicon nitride with elongated...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Thermochimica Acta

سال: 2021

ISSN: ['1872-762X', '0040-6031']

DOI: https://doi.org/10.1016/j.tca.2020.178807