Low cycle fatigue of a single crystal CoNi-base superalloy

نویسندگان

چکیده

The low cycle fatigue response of a single crystal γ′-containing CoNi-base superalloy has been investigated in air and vacuum at 950 °C. performance is demonstrated to be similar the 1st-generation Ni-base AM1. Fracture surface imaging cross-sections on both alloys reveal that oxidation-assisted cracking responsible for crack initiation air. improves under as transitions internal casting pores retained from solidification process. Recrystallized regions fracture surfaces vacuum-tested samples are identified by electron backscattered diffraction, which not previously reported these test conditions. role base element (Ni- vs. CoNi- Co-base) discussed.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Modelling of constitutive and fatigue behaviour of a single-crystal nickel-base superalloy

In this licentiate thesis the work done in the project KME410 will be presented. The overall objective of this project is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical behaviour of the material. The constitu...

متن کامل

Fatigue crack initiation in a notched single-crystal superalloy component

In this paper, the fatigue crack initiation in notched single-crystal test specimens of material MD2 is investigated and analysed. A critical plane approach is adopted, in which the total strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to describe the number of cycles to fatigue crack initiation. This relation is determined from a...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Science and Engineering A-structural Materials Properties Microstructure and Processing

سال: 2021

ISSN: ['0921-5093', '1873-4936']

DOI: https://doi.org/10.1016/j.msea.2021.142007