Laser Welding Of Finned Tubes Made Of Austenitic Steels
نویسندگان
چکیده
منابع مشابه
Laser Beam Welding of Austenitic-Ferritic Transition Joints
Transition joints between austenitic stainless steels and ferritic low alloy steels are extensively utilized in many high-temperature applications in energy conversion systems. Problems related to the use of such dissimilar metal welds (DMWs) have long been recognized, because of premature failures often occurring during service, connected to thermal stresses generated at the weld interface and...
متن کاملLaser welding of modern automotive high strength steels
The paper demonstrates the correlation between the chemical composition of steel grades and the hardness as well as the formability of laser welds generated with modern automotive high strength steel grades. At the very low heat input of industrial laser welding and the resulting extremely high cooling rate, the weld hardness is fully controlled by the carbon content of the base materials and n...
متن کاملLow-Temperature Carburization of Austenitic Stainless Steels
LOW-TEMPERATURE CARBURIZATION is a gaseous carburization process performed at atmospheric pressure, at temperatures where the kinetics of substitutional diffusion are very slow. Low-temperature carburization hardens the surface of austenitic stainless steels through the diffusion of interstitial carbon, without the formation of carbides. The surface must be activated, by modification and remova...
متن کاملDevelopment of Alumina-Forming Austenitic Stainless Steels
This paper presents the results of the continued development of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys, which exhibit a unique combination of excellent oxidation resistance via protective alumina (Al2O3) scale formation and high-temperature creep strength through the formation of stable nano-scale MC carbides and intermetallic precipitates. Efforts in fiscal ye...
متن کاملDissimilar laser welding of NiTi shape memory alloy to austenitic stainless steel archwires
In this research, dissimilar welding of NiTi shape memory alloy to AISI 304 austenitic stainless steel Archwires was investigated. For this purpose, common straight orthodontic archwire with rectangular cross-section and dimensions of (0.635 × 0.432 mm) were selected and the laser welding technique was used to connect the wires. The microstructure, chemical composition and phasesin the weld zon...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Archives of Metallurgy and Materials
سال: 2015
ISSN: 2300-1909
DOI: 10.1515/amm-2015-0309