Laser powder bed fusion of Ti6Al4V-xCu: Process parameters

نویسندگان

چکیده

The original intent of coating biomedical and surgical devices surface with antibacterial agents is to prevent infections. However, the difference in material properties between materials causes spall from devices. To address situation, current research focused on investigating possibility using laser powder bed fusion process a subset additive manufacturing technology situ alloy 1 at% Cu Ti6Al4V. In alloying Ti6Al4V would lead production medical inbuilt property. determine optimum parameters that could be used manufacture Ti6Al4V- alloy, single tracks were produced over wide range powers scanning speeds analyzed. Process 170 W, 1.0 ms-1 hatch distance 80 µm identified as possible for alloy. Rescanning was good strategy improve roughness, homogeneity concentration matrix.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Functionalization of Biomedical Ti6Al4V via In Situ Alloying by Cu during Laser Powder Bed Fusion Manufacturing

The modern medical industry successfully utilizes Laser Powder Bed Fusion (LPBF) to manufacture complex custom implants. Ti6Al4V is one of the most commonly used biocompatible alloys. In surgery practice, infection at the bone-implant interface is one of the key reasons for implant failure. Therefore, advanced implants with biocompatibility and antibacterial properties are required. Modificatio...

متن کامل

Thermographic Measurements of the Commercial Laser Powder Bed Fusion Process at NIST.

Measurement of the high-temperature melt pool region in the laser powder bed fusion (L-PBF) process is a primary focus of researchers to further understand the dynamic physics of the heating, melting, adhesion, and cooling which define this commercially popular additive manufacturing process. This paper will detail the design, execution, and results of high speed, high magnification in-situ the...

متن کامل

Measurement of the Melt Pool Length during Single Scan Tracks in a Commercial Laser Powder Bed Fusion Process

Contact author: [email protected] Certain commercial equipment, instruments, or materials are identified in this paper in order to specify the experimental procedure adequately. Such identification is not intended to imply recommendation or endorsement by the National Institute of Standards and Technology, nor is it intended to imply that the materials or equipment identified are necessari...

متن کامل

Study of the Microstructure and Cracking Mechanisms of Hastelloy X Produced by Laser Powder Bed Fusion

Hastelloy X (HX) is a Ni-based superalloy which suffers from high crack susceptibility during the laser powder bed fusion (LPBF) process. In this work, the microstructure of as-built HX samples was rigorously investigated to understand the main mechanisms leading to crack formation. The microstructural features of as-built HX samples consisted of very fine dendrite architectures with dimensions...

متن کامل

Laser powder bed fusion of Ti-6Al-4V parts: Thermal modeling and mechanical implications

A continuum-scale modeling approach is developed and employed with three-dimensional finite element analysis (FEA), for simulating the temperature response of a Ti-6Al-4V, two-layered parallelepiped with dimensions of 10×5×0.06 mm during Laser Powder Bed Fusion (L-PBF), a metals additive manufacturing (AM) method. The model has been validated using experimental melt pool measurements from the l...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of metals, materials and minerals

سال: 2021

ISSN: ['0857-6149']

DOI: https://doi.org/10.55713/jmmm.v31i2.1051