The suitability of the direct energy deposition process exothermic powders Fe-Ti in joining dissimilar metals to produce small parts a complete shape for various applications is considered. procedure commercial pure iron and titanium proportions modes are described. Optical microscopy SEM with EDX analysis, X-ray microhardness measurements laser-fabricated intermetallics applied. Intermetallic compounds FeTi, Fe2Ti, eutectoids, complex oxides nitrides, carbides found. Interlayer trans-layer cracks pores observed. A growth from 150 HV 900 was obtained all samples due precipitation brittle intermetallic phases gradient system during DED. dispersion values becomes significant Ti-rich areas; there, revealed structure features considered relation published results explained. Increased concentrations Ti + Fe = 3:1 on Fe- -substrate 1:1 1:3 lead increasing hardness its distribution, but also increases residual microstress. Recommendations given reduce power layers apply Fe-substrate, which can stress, pores, cracks.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

IN-SITU FABRICATION PROCESS OF AL- TIC COMPOSITE BY SLAG

The new in situ method for AI-TiC composite fabrication has been carried out. In this method, fabrication of AI-TiC composite by simultaneous introduction of titanium oxide and carbon into aluminum melt was investigated.. Under the process conditions, titanium and carbon reaction results in titanium carbide whiskers. The salt containing keriolite (Na3AIF6), titanium oxide (TiO2) and graphite us...

متن کامل

Experimental Analysis of the Direct Laser Metal Deposition Process

In the current economic situation, with a liberalized and worldwide trade, the weight of time and costs reduction for developing new products increases. In particular, the tooling processes, which are already expensive and time consuming, recently became a critical trouble. The geometric complexity, the number of variants and the amount of requirements that characterize the products that are re...

متن کامل

Production of Fe-TiN and Fe-Ti(N,C) composite powders by mechanical alloying

In this research, the production of Fe-TiN and Fe-Ti(N,C) composite powders by mechanical alloying was investigated and evaluated. Ferrotitanium (containing 70%Ti), titanium and graphite were used as the raw materials. Initial mixtures were milled in different time durations under the pure nitrogen atmosphere with the pressure of 5atm. The results showed that when N2 pressure is 5 at...

متن کامل

DIRECT LASER DEPOSITION OF Ti-6Al-4V FROM ELEMENTAL POWDER BLENDS

A thin-wall structure composed of Ti-6Al-4V has been deposited using direct laser deposition (DLD) from blended Ti, Al, and V elemental powders. The microstructure and composition distribution along the build height direction were intensively investigated using optical microscopy, scanning electron microscopy/energy dispersive X-ray spectroscopy (SEM/EDS), and Vickers hardness testing. The micr...

متن کامل

Synthesis of Fe-Al-Ti Based Intermetallics with the Use of Laser Engineered Net Shaping (LENS)

The Laser Engineered Net Shaping (LENS) technique was combined with direct synthesis to fabricate L21-ordered Fe-Al-Ti based intermetallic alloys. It was found that ternary Fe-Al-Ti alloys can be synthesized using the LENS technique from a feedstock composed of a pre-alloyed Fe-Al powder and elemental Ti powder. The obtained average compositions of the ternary alloys after the laser deposition ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of manufacturing and materials processing

سال: 2023

ISSN: ['2504-4494']

DOI: https://doi.org/10.3390/jmmp7020066