Karakteristik Laju Regangan Melar pada Baja Tahan Karat Austenitic 316L

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue behavior of Austenitic Type 316L Stainless Steel

The aim of this work is to determine the fatigue life of 316L stainless steel. The mechanisms of fatigue of 316L stainless steels were investigated and discussed. The fatigue tests were carried out at constant-amplitude cyclic loading with load ratio R=0.1. Scanning Electron Microscope (SEM) is then used to examine the fracture surface. The results show that the fatigue limit of 316L stainless ...

متن کامل

HYDRAULIC BEHAVIOR IN THE DOWNFLOW HANGING SPONGE BIOREACTOR Karakteristik Hidraulik pada Bioreactor Downflow Hanging Sponge

Performance efficiency in a Downflow Hanging Sponge (DHS) bioreactor is associated with the amount of time that a wastewater remains in the bioreactor. The bioreactor is considered as a plug flow reactor and its hydraulic residence time (HRT) depends on the void volume of packing material and the flow rate. In this study, hydraulic behavior of DHS bioreactor was investigated by using tracer met...

متن کامل

Improvement in the Corrosion Resistance of Austenitic Stainless Steel 316L by Ion Implantation*

In the present work, austenitic stainless steel 316L (SS316L) samples were implanted with Ni and Ni-Cr. A nickel-rich layer about 100 nm in thickness and a Ni-Cr enriched layer about 60 nm thick are formed on the surface of SS316L. The effects of ion implantation on the corrosion performance of SS316L are investigated in a 0.5 M H2SO4 with 2 ppm HF solution at 80°C by open circuit potential (OC...

متن کامل

Haemocompatibility of Surface Modified AISI 316L Austenitic Stainless Steel Tested in Artificial Plasma

The study comprises evaluation of suitability of passive layer created on the surface of AISI 316L stainless steel for products that are intended to have contact with blood. For that purpose, prior to and after chemical passivation, samples were subject to 7 day exposure in artificial plasma at the temperature of T=37°C. Next, tests of metallic ions infiltration from the surface to the solution...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: ROTASI

سال: 2017

ISSN: 2406-9620,1411-027X

DOI: 10.14710/rotasi.19.4.201-205